AW-2117 T4 Aluminum Copper Alloy – EN 573-3 Certified
Age-hardenable AlCu alloy. The alloy is not food safe.
Properties
General
| Property | Temperature | Value | Condition | Related Standards | Shape |
|---|---|---|---|---|---|
Density | 2.75 g/cm³ | T4 | EN 573-3, EN 1301 | Wire | |
20.0 °C | 2.74 g/cm³ | T4 | EN 573-3 | Wire |
Mechanical
| Property | Temperature | Value | Condition | Related Standards | Shape | Comment |
|---|---|---|---|---|---|---|
Elastic modulus | 70.0 GPa | T4 | EN 573-3, EN 1301 | Wire | ||
20.0 °C | 67.0 GPa | T4 | EN 573-3 | Wire | ||
Elongation | 20.0 % | T4 | EN 573-3, EN 1301 | Wire | ||
20.0 °C | 5.0 % | T4 | EN 573-3 | Wire | A100 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m | Typical for Wrought 2000 Series Aluminium | ||||
Poisson's ratio | 0.33 [-] | Typical for Wrought 2000 Series Aluminium | ||||
Shear modulus | 20.0 °C | 25.5 GPa | T4 | EN 573-3 | Wire | |
Tensile strength | 260.0 MPa | T4 | EN 573-3, EN 1301 | Wire | ||
20.0 °C | 170.0 - 240.0 MPa | T4 | EN 573-3 | Wire |
Thermal
| Property | Temperature | Value | Condition | Related Standards | Shape |
|---|---|---|---|---|---|
Coefficient of thermal expansion | -50.0 °C | 2.18e-05 1/K | T4 | EN 573-3 | Wire |
20 °C | 2.38e-05 1/K | T4 | EN 573-3, EN 1301 | Wire | |
100.0 °C | 2.34e-05 1/K | T4 | EN 573-3 | Wire | |
100 °C | 2.38e-05 1/K | T4 | EN 573-3, EN 1301 | Wire | |
200.0 °C | 2.45e-05 1/K | T4 | EN 573-3 | Wire | |
300.0 °C | 2.56e-05 1/K | T4 | EN 573-3 | Wire | |
Melting point | 550.0 - 650.0 °C | T4 | EN 573-3, EN 1301 | Wire | |
Specific heat capacity | 20.0 °C | 898.0 J/(kg·K) | T4 | EN 573-3 | Wire |
Thermal conductivity | 155 W/(m·K) | T4 | EN 573-3, EN 1301 | Wire | |
20.0 °C | 150.0 - 180.0 W/(m·K) | T4 | EN 573-3 | Wire |
Electrical
| Property | Temperature | Value | Condition | Related Standards | Shape |
|---|---|---|---|---|---|
Electrical conductivity | 23000000.0 S/m | T4 | EN 573-3, EN 1301 | Wire | |
20.0 °C | 21000000.0 - 25000000.0 S/m | T4 | EN 573-3 | Wire | |
Electrical resistivity | 4.35e-08 Ω·m | T4 | EN 573-3, EN 1301 | Wire |
Chemical properties
| Property | Value | Condition | Related Standards | Shape |
|---|---|---|---|---|
Chromium | 0.1 % | T4 | EN 573-3, EN 1301 | Wire |
Copper | 2.2 - 3.0 % | T4 | EN 573-3, EN 1301 | Wire |
Iron | 0.7 % | T4 | EN 573-3 | Wire |
0.70 % | T4 | EN 573-3, EN 1301 | Wire | |
Magnesium | 0.2 - 0.5 % | T4 | EN 573-3, EN 1301 | Wire |
Manganese | 0.2 % | T4 | EN 573-3, EN 1301 | Wire |
Silicon | 0.8 % | T4 | EN 573-3, EN 1301 | Wire |
Zinc | 0.25 % | T4 | EN 573-3, EN 1301 | Wire |
Technological properties
| Property | ||
|---|---|---|
| Brazing | hard brazing (with flux/ without flux): sufficient / sufficient | |
| Corrosion properties | Seawater: poor, weathering: poor | |
| Workability | Moderate Workability | |
Metal
- EN 573-3 Grade 3.0505 F Aluminium Alloy: Properties & Standards
- EN 573-3 Grade 3.1305 F Aluminium Alloy – Key Mechanical Properties
- EN 573-3 Grade 3.1305 O Aluminium: Key Mechanical Properties & Standards
- EN 573-3 Grade 3.1305 O3 – Comprehensive Aluminium Alloy Specifications
- EN 573-3 Grade 3.3316 F – Key Properties & Standards for 5000 Series Aluminium
- EN 573-3 Grade AW-2117 O – Standard Aluminium Wire Properties
- EN 573-3 Certified AW-2117 O3 Aluminium Alloy – Technical Specifications
- AW-2117 F – Premium EN 573-3 Certified Aluminium Alloy for Industrial Engineering
- AW-2117 H18: Premium Age-Hardenable AlCu Alloy (EN 573-3 Grade)
- EN 573-3 Grade AW-2117 H13 – Premium Age‑Hardenable AlCu Alloy