ASTM A803 Grade 25-4-4 Solution-Annealed: High-Strength Ferritic Stainless Steel
Properties
General
| Property | Temperature | Value | Comment |
|---|---|---|---|
Density | 23.0 °C | 7.6 - 7.8 g/cm³ | Typical for Ferritic Stainless Steel |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 23.0 °C | 220 GPa | Typical for Ferritic Stainless Steel |
Elongation A50 | 23.0 °C | 20 % | |
Hardness, Brinell | 23.0 °C | 270 [-] | |
Hardness, Rockwell B | 23.0 °C | 27 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] | Typical for Ferritic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa | Typical for Ferritic Stainless Steel |
Tensile strength | 23.0 °C | 620 MPa | |
Yield strength | 23.0 °C | 515 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 9.3E-6 - 1.2E-5 1/K | Typical for Ferritic Stainless Steel |
Melting point | 1425 - 1530 °C | Typical for Ferritic Stainless Steel | |
Specific heat capacity | 23.0 °C | 420 - 586 J/(kg·K) | Typical for Ferritic Stainless Steel |
Thermal conductivity | 23.0 °C | 11 - 22 W/(m·K) | Typical for Ferritic Stainless Steel |
Electrical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Electrical resistivity | 23.0 °C | 6E-7 - 7.5E-7 Ω·m | Typical for Ferritic Stainless Steel |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.025 % |
Chromium | 24.5 - 26 % |
Manganese | 1 % |
Molybdenum | 3.5 - 4.5 % |
Nickel | 3.5 - 4.5 % |
Nitrogen | 0.04 % |
Phosphorus | 0.04 % |
Silicon | 0.75 % |
Sulfur | 0.03 % |
Titanium | 0.8 % |
Metal
- ASTM A803 Grade 29‑4 Solution‑Annealed Ferritic Stainless Steel – Properties & Specifications
- ASTM A803 Grade 29-4C – Solution-Annealed Ferritic Stainless Steel
- ASTM A803 TP409 – High-Performance Solution-Annealed Ferritic Stainless Steel
- ASTM A803 TPXM-27 Solution‑Annealed Stainless Steel – Premium Ferritic Grade
- ASTM A803 Grade 18-2 Solution-Annealed Stainless Steel – Key Properties
- ASTM A803 Grade 26-3-3 Solution-Annealed Stainless Steel – Premium Ferritic Performance
- ASTM A803 Grade 29-4-2 – Solution-Annealed Stainless Steel: Properties & Specs
- ASTM A803 TP439 Solution-Annealed Stainless Steel – Detailed Properties & Performance
- ASTM A803 Grade TPXM-33 – Solution-Annealed Ferritic Stainless Steel
- ASTM A268 Grade 25-4-4 Reheated Stainless Steel – Key Properties & Specifications