| Property | Temperature | Value | Comment |
|---|---|---|---|
Density | 23.0 °C | 7.9 - 8.2 g/cm³ | Typical for Austenitic Stainless Steel |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 23.0 °C | 195 GPa | Typical for Austenitic Stainless Steel |
Elongation A50 | 23.0 °C | 30 % | |
Hardness, Brinell | 23.0 °C | 217 [-] | |
Hardness, Rockwell B | 23.0 °C | 95 [-] | |
Poisson's ratio | 23.0 °C | 0.3 [-] | Typical for Austenitic Stainless Steel |
Shear modulus | 23.0 °C | 77 GPa | Typical for Austenitic Stainless Steel |
Tensile strength | 23.0 °C | 550 MPa | |
Yield strength | 23.0 °C | 240 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 1.9E-5 1/K | Typical for Austenitic Stainless Steel |
Melting point | 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | 23.0 °C | 440 J/(kg·K) | Typical for Austenitic Stainless Steel |
Thermal conductivity | 23.0 °C | 11 - 21 W/(m·K) | Typical for Austenitic Stainless Steel |
Electrical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Electrical resistivity | 23.0 °C | 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.07 % |
Chromium | 19 - 21 % |
Manganese | 2 % |
Molybdenum | 2 - 3 % |
Nickel | 32 - 38 % |
Phosphorus | 0.05 % |
Silicon | 1 % |
Sulfur | 0.035 % |
Metal
- ASTM A214 Grade A214 Heat‑Treated Steel: Key Properties & Specifications
- ASTM A240 Grade S40920 Heat‑Treated Stainless Steel – Premium Ferritic Properties
- ASTM A240 Grade S40930 Heat‑Treated Stainless Steel – Premium Performance
- ASTM A240 S40975 Heat‑Treated Ferritic Stainless Steel – Key Properties
- ASTM A240 Grade S41003 – Heat‑Treated Ferritic Stainless Steel – Key Mechanical & Physical Properties
- ASTM A551 Class CHT Heat‑Treated Steel: Properties & Performance
- ASTM A551 Class DHT Heat-Treated Steel – Key Properties & Performance
- Heat‑Treated TP310S Austenitic Stainless Steel – ASTM A249 Standard
- ASTM Alloy 20 Heat‑Treated Stainless Steel – Properties & Performance
- ASTM A335 Grade P1 Heat‑Treated Steel – Properties & Performance