EN 12166 Copper Alloy Grade CuZn37Pb2 H100 – Specifications & Properties
Wire fom copper alloy for general purposes.
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.4 - 8.45 g/cm³ |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 20.0 °C | 105 GPa | |
Hardness, Brinell | 20.0 °C | 100 - 140 [-] | |
Hardness, Vickers | 20.0 °C | 100 - 150 [-] | |
Shear modulus | 23.0 °C | 40 GPa | Typical for Wrought Copper Brass |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Melting point | 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 23.0 °C | 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Thermal conductivity | 20.0 °C | 105 W/(m·K) |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 1.40E+7 S/m |
Specific Electrical conductivity | 24 % IACS |
Chemical properties
| Property | Value |
|---|---|
Aluminium | 0.05 % |
Copper | 61 - 62 % |
Iron | 0.2 % |
Lead | 1.6 - 2.5 % |
Nickel | 0.3 % |
Tin | 0.2 % |
Metal
- EN 12166 Grade CuNi18Zn20 H01 – High Strength, Corrosion-Resistant Copper–Nickel–Zinc Alloy
- EN 12166 Copper Brass Grade CuZn15 R310 – Specifications & Properties
- EN 12166 CuZn30 H00 Wrought Copper Alloy – Superior Strength and Corrosion Resistance
- EN 12166 CuZn39Pb0.5 H100 Copper Alloy Wire – Specifications & Properties
- EN 12166 CuZn37Pb2 H125 Copper Alloy – High-Strength, Corrosion-Resistant Profiles
- EN 12166 Grade CuZn37Pb2 (H070) – Premium Copper Alloy Profiles & Bars
- EN 12166 Grade CuZn38Pb2 H100 – High-Quality Copper Alloy Wire for Industrial Applications
- EN 12166: Grade CuZr M – Premium Low‑Alloy Copper with Superior Strength and Conductivity
- EN 12166 Grade CuBe2 TD – Premium Hardenable Copper-Beryllium Alloy
- EN 12166 Grade CuZn39Pb2 H100 – Leaded Brass Alloy Specifications