EN 12166 Grade CuBe2 TD – Premium Hardenable Copper-Beryllium Alloy
CuBe2, mat. No CW101C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuBe2, mat. No 2.1247, acc. to DIN 17666 : 1983-12 applies: It is an alloy of optimal hardenability for highest requirements to strength, elasticity, abrasion and fatigue resistance. CuBe2 shows mean electrical and favorable thermal conductivity. The material does not show any embrittlement at lower temperatures (up to -200°C) as well as no stress corrosion sensitivity. The temperature for removal of workhardening approximates 350°C. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: For bearing jewels and screws, tensioning belts and wires, membranes, balance springs and drawn parts for watches, all types of springs. Individual parts for HF- and NF- special couplers, wear-resistant worms and gear-wheels, high-stress solid components, non-magnetic and spark-safe. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.3 g/cm³ |
Mechanical
| Property | Temperature | Value |
|---|---|---|
Elastic modulus | 20.0 °C | 135 GPa |
Elongation | 20.0 °C | 8 - 20 % |
Elongation A50 | 20.0 °C | 2 - 35 % |
Hardness, Vickers | 20.0 °C | 90 - 290 [-] |
Tensile strength | 20.0 °C | 410 - 830 MPa |
Yield strength Rp0.2 | 20.0 °C | 190 - 800 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.7E-5 1/K | |
Melting point | 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 23.0 °C | 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Thermal conductivity | 20.0 °C | 92 - 125 W/(m·K) |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 8.00E+6 - 1.80E+7 S/m |
Specific Electrical conductivity | 23 % IACS |
Chemical properties
| Property | Value |
|---|---|
Beryllium | 1.8 - 2.1 % |
Cobalt | 0.3 % |
Iron | 0.2 % |
Nickel | 0.3 % |
Metal
- EN 12166 Grade CuNi18Zn20 H01 – High Strength, Corrosion-Resistant Copper–Nickel–Zinc Alloy
- EN 12166 Copper Brass Grade CuZn15 R310 – Specifications & Properties
- EN 12166 CuZn30 H00 Wrought Copper Alloy – Superior Strength and Corrosion Resistance
- EN 12166 Grade CuZn36 R360 – Premium Beryllium Copper Alloy
- EN 12163 Grade CuBe2 M: High-Performance Hardenable Copper Alloy
- EN 12166 Grade CuBe2 R1300 – Premium Copper‑Beryllium Alloy for Wire, Springs & Fasteners
- EN 12165 Grade CuBe2 M – Premium Hardenable Copper Alloy for High Strength and Durability
- EN 12166 Grade CuBe2 R1150: Premium Copper‑Beryllium Alloy for Wire & Fasteners
- EN 12166: Grade CuZr M – Premium Low‑Alloy Copper with Superior Strength and Conductivity
- EN 1652 Grade CuBe2 TH: High-Performance Hardenable Copper Alloy