EN 12163 Grade CuBe2 M: High-Performance Hardenable Copper Alloy
CuBe2, mat. No CW101C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuBe2, mat. No 2.1247, acc. to DIN 17666 : 1983-12 applies: It is an alloy of optimal hardenability for highest requirements to strength, elasticity, abrasion and fatigue resistance. CuBe2 shows mean electrical and favorable thermal conductivity. The material does not show any embrittlement at lower temperatures (up to -200°C) as well as no stress corrosion sensitivity. The temperature for removal of workhardening approximates 350°C. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: For bearing jewels and screws, tensioning belts and wires, membranes, balance springs and drawn parts for watches, all types of springs. Individual parts for HF- and NF- special couplers, wear-resistant worms and gear-wheels, high-stress solid components, non-magnetic and spark-safe. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.3 g/cm³ |
Mechanical
| Property | Temperature | Value |
|---|---|---|
Elastic modulus | 20.0 °C | 135 GPa |
Hardness, Brinell | 20.0 °C | 80 - 420 [-] |
Hardness, Vickers | 20.0 °C | 90 [-] |
Tensile strength | 20.0 °C | 410 - 450 MPa |
Yield strength Rp0.2 | 20.0 °C | 190 - 200 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 300.0 °C | 1.7E-5 1/K | |
Melting point | 855 - 1090 °C | Typical for Wrought Copper High Copper Alloy | |
Specific heat capacity | 23.0 °C | 360 - 420 J/(kg·K) | Typical for Wrought Copper High Copper Alloy |
Thermal conductivity | 20.0 °C | 92 - 125 W/(m·K) |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 8.00E+6 - 1.80E+7 S/m |
Chemical properties
| Property | Value |
|---|---|
Beryllium | 1.8 - 2.1 % |
Cobalt | 0.3 % |
Iron | 0.2 % |
Nickel | 0.3 % |
Metal
- EN 12163 Grade CuBe2 H350 – High‑Strength, Low‑Temperature Copper Alloy
- EN 12163 CuZr TH Grade – High Strength Low‑Alloy Copper Alloy
- EN 12163 Grade CuZn10 M – High-Strength, Corrosion-Resistant Copper Alloy
- EN 12163 CuZn40 M: High-Performance Unhardenable Wrought Copper Alloy
- EN 12163: Grade CuZn33 M – High-Strength Unhardenable Wrought Copper Alloy
- EN 12165 Grade CuBe2 M – Premium Hardenable Copper Alloy for High Strength and Durability
- EN 12163 Grade CuZn36 M – Premium Unhardenable Copper Alloy for Precision Deep Drawing
- EN 12163 Grade CuBe2 R1150 – Premium Hardenable Copper Alloy for High Strength & Thermal Performance
- EN 12163 Grade CuBe2 R1300 – High-Strength Hardenable Copper Alloy
- EN 12166 Grade CuBe2 TD – Premium Hardenable Copper-Beryllium Alloy