CuBe2, mat. No CW101C, is counted among hardenable, low alloyed copper alloys. To the comparable make CuBe2, mat. No 2.1247, acc. to DIN 17666 : 1983-12 applies: It is an alloy of optimal hardenability for highest requirements to strength, elasticity, abrasion and fatigue resistance. CuBe2 shows mean electrical and favorable thermal conductivity. The material does not show any embrittlement at lower temperatures (up to -200°C) as well as no stress corrosion sensitivity. The temperature for removal of workhardening approximates 350°C. Processing properties: hot and cold forming: good machinability: moderately hard and soft soldering: good gas shielded welding: good burnishing: good Application: For bearing jewels and screws, tensioning belts and wires, membranes, balance springs and drawn parts for watches, all types of springs. Individual parts for HF- and NF- special couplers, wear-resistant worms and gear-wheels, high-stress solid components, non-magnetic and spark-safe. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.3 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

135 GPa

Elongation

20.0 °C

2 %

Tensile strength

20.0 °C

1150 MPa

Yield strength Rp0.2

20.0 °C

1000 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

300.0 °C

1.7E-5 1/K

Melting point

855 - 1090 °C

Typical for Wrought Copper High Copper Alloy

Specific heat capacity

23.0 °C

360 - 420 J/(kg·K)

Typical for Wrought Copper High Copper Alloy

Thermal conductivity

20.0 °C

92 - 125 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

8.00E+6 - 1.80E+7 S/m

Specific Electrical conductivity

26 % IACS

Chemical properties

PropertyValue

Beryllium

1.8 - 2.1 %

Cobalt

0.3 %

Iron

0.2 %

Nickel

0.3 %


Metal

  1. EN 12163 Grade CuBe2 H350 – High‑Strength, Low‑Temperature Copper Alloy
  2. EN 12163 CuZr TH Grade – High Strength Low‑Alloy Copper Alloy
  3. EN 12163 Grade CuBe2 M: High-Performance Hardenable Copper Alloy
  4. EN 12163 Grade CuZn10 M – High-Strength, Corrosion-Resistant Copper Alloy
  5. EN 12163 CuZn40 M: High-Performance Unhardenable Wrought Copper Alloy
  6. EN 12163: Grade CuZn33 M – High-Strength Unhardenable Wrought Copper Alloy
  7. EN 12165 Grade CuBe2 M – Premium Hardenable Copper Alloy for High Strength and Durability
  8. EN 12166 Grade CuBe2 R1150: Premium Copper‑Beryllium Alloy for Wire & Fasteners