EN 1652 Copper Brass CuZn38Pb2 R340 – Specifications & Performance
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.4 - 8.44 g/cm³ |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 20.0 °C | 102 GPa | |
Elongation | 20.0 °C | 43 % | |
Elongation A50 | 20.0 °C | 33 % | |
Poisson's ratio | 20.0 °C | 0.34 [-] | |
Shear modulus | 23.0 °C | 40 GPa | Typical for Wrought Copper Brass |
Tensile strength | 20.0 °C | 340 - 420 MPa | |
Yield strength Rp0.2 | 20.0 °C | 240 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 2E-5 1/K | |
300.0 °C | 2.1E-5 1/K | ||
Melting point | 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 20.0 °C | 377 J/(kg·K) | |
Thermal conductivity | 20.0 °C | 109 - 110 W/(m·K) | |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 1.39E+7 - 1.40E+7 S/m |
Specific Electrical conductivity | 24 % IACS |
Chemical properties
| Property | Value |
|---|---|
Aluminium | 0.05 % |
Copper | 60 - 61 % |
Iron | 0.2 % |
Lead | 1.6 - 2.5 % |
Nickel | 0.3 % |
Tin | 0.2 % |
Metal
- EN 1652 CuCo1Ni1Be TH – High-Performance Copper Alloy for Industrial Applications
- EN 1652 Grade CuZn38Pb2 H110 – Premium Wrought Copper Brass
- EN 1652 Grade CuZn38Pb2 R400 – Specifications & Properties
- EN 1652 Grade CuSn6 M – Premium Tin-Copper Alloy for Superior Corrosion Resistance
- EN 1652 Grade CuNi2Si M – High-Performance Copper Alloy for Superior Conductivity and Corrosion Resistance
- EN 1652 Grade CuNi9Sn2 R340: High‑Strength, Tarnish‑Resistant Alloy for Superior Performance
- EN 1652 CuZn5 R340 – High-Conductivity, Corrosion-Resistant Alloy
- EN 1652 Copper Alloy CuZn38Pb2 R470 – High-Performance Seamless Round Tubes
- EN 1652 CuZn39Pb0.5 R340: Unhardenable Wrought Brass Alloy with Enhanced Machinability
- EN 1652 CuZn40 R340: High-Strength, Low-Conductivity Wrought Copper Alloy