EN 12166 CuZn39Pb0.5 Copper Alloy – H120 – Premium Profiles & Bars
Copper alloy profiles and bars for general purposes.
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.4 g/cm³ |
Mechanical
| Property | Temperature | Value |
|---|---|---|
Elastic modulus | 20.0 °C | 102 GPa |
Hardness, Brinell | 20.0 °C | 120 [-] |
Hardness, Vickers | 20.0 °C | 125 [-] |
Shear modulus | 20.0 °C | 37 GPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 200.0 °C | 2.04E-5 1/K | |
Melting point | 875 - 1075 °C | Typical for Wrought Copper Brass | |
Specific heat capacity | 23.0 °C | 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Thermal conductivity | 20.0 °C | 109 W/(m·K) |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 1.39E+7 S/m |
Electrical resistivity | 20.0 °C | 7.2E-8 Ω·m |
Chemical properties
| Property | Value |
|---|---|
Aluminium | 0.05 % |
Copper | 59 - 60.5 % |
Iron | 0.2 % |
Lead | 0.2 - 0.8 % |
Nickel | 0.3 % |
Tin | 0.2 % |
Metal
- EN 12166 Grade CuNi18Zn20 H01 – High Strength, Corrosion-Resistant Copper–Nickel–Zinc Alloy
- EN 12166 Copper Brass Grade CuZn15 R310 – Specifications & Properties
- EN 12166 CuZn30 H00 Wrought Copper Alloy – Superior Strength and Corrosion Resistance
- EN 12166 Grade CuZn36 R360 – Premium Beryllium Copper Alloy
- EN 12166 Grade CuNi10Zn27 H01: High-Performance Copper-Nickel-Zinc Alloy Wire
- EN 12166 Grade CuNi10Zn27 O60: High-Performance Copper-Nickel-Zinc Wire
- EN 12166 CuZn39Pb0.5 H100 Copper Alloy Wire – Specifications & Properties
- EN 12166: Grade CuZr M – Premium Low‑Alloy Copper with Superior Strength and Conductivity
- EN 12166 Grade CuBe2 TD – Premium Hardenable Copper-Beryllium Alloy
- EN 12166 CuZn39Pb0.5 R500 Wire – High‑Strength, High‑Conductivity Copper Alloy