CuSn6, mat. No. CW425K, is comparable to the DIN-make CuSn6, mat. No. 2.1020, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Appliction: For all types of springs, especially in electrical industry, for connectors, hose and spring tubes, fabric and screening wires, gong bars. Further application in paper, cellulose and chemical industry, in shipbuilding and machine engineering. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.8 - 8.82 g/cm³ |
Mechanical
| Property | Temperature | Value |
|---|---|---|
Elastic modulus | 20.0 °C | 118 GPa |
Hardness, Brinell | 20.0 °C | 120 - 155 [-] |
Hardness, Vickers | 20.0 °C | 125 - 155 [-] |
Poisson's ratio | 20.0 °C | 0.34 [-] |
Thermal
| Property | Temperature | Value |
|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.8E-5 1/K |
200.0 °C | 1.85E-5 1/K | |
650.0 °C | 2.22E-5 1/K | |
800.0 °C | 2.18E-5 1/K | |
Max service temperature, long | 0 - 150 °C | |
Specific heat capacity | 20.0 °C | 377 J/(kg·K) |
Thermal conductivity | 20.0 °C | 75 W/(m·K) |
200.0 °C | 98 W/(m·K) | |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 9.00E+6 S/m |
200.0 °C | 7.80E+6 S/m | |
Electrical resistivity | 20.0 °C | 1.11E-7 Ω·m |
200.0 °C | 1.28E-7 Ω·m | |
Specific Electrical conductivity | 16 % IACS | |
Chemical properties
| Property | Value |
|---|---|
Iron | 0.1 % |
Lead | 0.02 % |
Nickel | 0.2 % |
Phosphorus | 0.01 - 0.4 % |
Tin | 5.5 - 7 % |
Zinc | 0.2 % |
Metal
- EN 12163 CuZr TH Grade – High Strength Low‑Alloy Copper Alloy
- EN 12163 CuZn39Sn1 (H120) – Premium Copper Alloy for Industrial Applications
- EN 12163 Grade H120 CuZr Copper Alloy – High Strength, Excellent Conductivity
- EN 12163 Grade CuZn35Ni3Mn2AlPb H120 – Premium Unhardenable Copper Alloy
- EN 12163 Grade CuSn6 H085: Premium Tin-Copper Alloy for High-Performance Applications
- EN 12163 Grade CuSn6 (H155) – High-Performance Tin-Copper Alloy
- EN 12163 CuSn6 R550 – Premium Copper‑Tin Alloy with Superior Corrosion Resistance
- EN 12163 Grade CuSn6 R470 – High-Performance Tin‑Copper Alloy
- EN 12163 Grade CuSn6 R400: Premium Tin‑Copper Alloy with Superior Corrosion Resistance
- EN 12163 Grade CuSn6 R340 – Premium Tin‑Copper Alloy for Superior Corrosion Resistance