CuSn6, mat. No. CW425K, is comparable to the DIN-make CuSn6, mat. No. 2.1020, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Appliction: For all types of springs, especially in electrical industry, for connectors, hose and spring tubes, fabric and screening wires, gong bars. Further application in paper, cellulose and chemical industry, in shipbuilding and machine engineering. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.8 - 8.82 g/cm³ |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Elongation A10 | 20.0 °C | 5 % | |
Elongation A100 | 20.0 °C | 4 % | |
Poisson's ratio | 23.0 °C | 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 20.0 °C | 550 MPa | |
Yield strength Rp0.2 | 20.0 °C | 500 MPa |
Thermal
| Property | Temperature | Value |
|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.8E-5 1/K |
200.0 °C | 1.85E-5 1/K | |
650.0 °C | 2.22E-5 1/K | |
800.0 °C | 2.18E-5 1/K | |
Max service temperature, long | 0 - 150 °C | |
Specific heat capacity | 20.0 °C | 377 J/(kg·K) |
Thermal conductivity | 20.0 °C | 75 W/(m·K) |
200.0 °C | 98 W/(m·K) | |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 9.00E+6 S/m |
200.0 °C | 7.80E+6 S/m | |
Electrical resistivity | 20.0 °C | 1.11E-7 Ω·m |
200.0 °C | 1.28E-7 Ω·m | |
Chemical properties
| Property | Value |
|---|---|
Iron | 0.1 % |
Lead | 0.02 % |
Nickel | 0.2 % |
Phosphorus | 0.01 - 0.4 % |
Tin | 5.5 - 7 % |
Zinc | 0.2 % |
Metal
- EN 12163 CuZr TH Grade – High Strength Low‑Alloy Copper Alloy
- EN 12163 Grade CuBe2 M: High-Performance Hardenable Copper Alloy
- EN 12163 Grade CuSn6 H085: Premium Tin-Copper Alloy for High-Performance Applications
- EN 12163 Grade CuSn6 H120 – Premium Tin-Copper Alloy for High-Performance Applications
- EN 12163 Grade CuSn6 (H155) – High-Performance Tin-Copper Alloy
- EN 12163 CuZn35Ni3Mn2AlPb R550: High-Performance Copper Alloy for Superior Strength and Corrosion Resistance
- EN 12163 Grade R550 CuNi2Si: High-Performance Copper Alloy
- EN 12163 Grade CuSn6 R470 – High-Performance Tin‑Copper Alloy
- EN 12163 Grade CuSn6 R400: Premium Tin‑Copper Alloy with Superior Corrosion Resistance
- EN 12163 Grade CuSn6 R340 – Premium Tin‑Copper Alloy for Superior Corrosion Resistance