EN 10132‑4 Grade 80CrV2 Quenched Steel (Q) – High‑Performance Spring & Cold‑Rolled Strip
The steel 80CrV2 is used as cold rolled strip for springs and special applications in thicknesses of up to 6 mm and as tempered cold strip in thicknesses from 0.30 to 3.00 mm.
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 7.81 g/cm³ |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | -100.0 °C | 217 GPa | |
20.0 °C | 212 GPa | ||
100.0 °C | 207 GPa | ||
200.0 °C | 199 GPa | ||
300.0 °C | 192 GPa | ||
400.0 °C | 184 GPa | ||
500.0 °C | 175 GPa | ||
600.0 °C | 164 GPa | ||
Hardness, Rockwell C | 20.0 °C | 60 [-] | |
Hardness, Vickers | 20.0 °C | 700 [-] | |
Poisson's ratio | 20.0 °C | 0.28 [-] | |
Shear modulus | 23.0 °C | 79 GPa | Typical for Tool And Machining Steel |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | -100.0 °C | 1.05E-5 1/K | |
20.0 °C | 1.15E-5 1/K | ||
100.0 °C | 1.21E-5 1/K | ||
200.0 °C | 1.27E-5 1/K | ||
300.0 °C | 1.32E-5 1/K | ||
400.0 °C | 1.36E-5 1/K | ||
500.0 °C | 1.4E-5 1/K | ||
600.0 °C | 1.44E-5 1/K | ||
Melting point | 1370 - 1425 °C | Typical for Tool And Machining Steel | |
Specific heat capacity | -100.0 °C | 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) | ||
Thermal conductivity | 20.0 °C | 39.6 W/(m·K) | |
100.0 °C | 41.6 W/(m·K) | ||
200.0 °C | 41.8 W/(m·K) | ||
300.0 °C | 40.3 W/(m·K) | ||
400.0 °C | 38.2 W/(m·K) | ||
500.0 °C | 36 W/(m·K) | ||
600.0 °C | 33.6 W/(m·K) | ||
Thermal diffusivity | 20.0 °C | 11 mm²/s | |
100.0 °C | 10.8 mm²/s | ||
200.0 °C | 10.1 mm²/s | ||
300.0 °C | 9.2 mm²/s | ||
400.0 °C | 8.1 mm²/s | ||
500.0 °C | 7 mm²/s | ||
600.0 °C | 5.7 mm²/s | ||
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical resistivity | 20.0 °C | 2.63E-7 Ω·m |
100.0 °C | 3.08E-7 Ω·m | |
200.0 °C | 3.78E-7 Ω·m | |
300.0 °C | 4.66E-7 Ω·m | |
400.0 °C | 5.69E-7 Ω·m | |
500.0 °C | 6.87E-7 Ω·m | |
600.0 °C | 8.26E-7 Ω·m | |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.75 - 0.85 % |
Chromium | 0.4 - 0.6 % |
Manganese | 0.3 - 0.5 % |
Molybdenum | 0.1 % |
Nickel | 0.4 % |
Phosphorus | 0.03 % |
Silicon | 0.15 - 0.35 % |
Sulfur | 0.025 % |
Vanadium | 0.15 - 0.25 % |
Metal
- EN 10132-4 Grade 51CrV4 Quenched Steel (Q) – High‑Performance Cold Rolled Strip
- EN 10132-4 Grade C55S Quenched Steel – High‑Performance Cold Rolled Strip for Springs & Precision Applications
- EN 10132-4 Grade C60S Quenched Steel – High-Performance Cold-Rolled Strip
- EN 10132-4 Grade C90S Quenched Steel – Optimal for Springs & Cold‑Rolled Strips
- EN 10132-4: 102Cr6 Steel – Quenched Grade for High-Performance Applications
- EN 10132-4 Grade 80CrV2 Steel: Quenched & Tempered (QT) – High-Performance Spring Strip
- EN 10132‑4 Grade C100S Quenched Steel for Springs and Precision Components
- EN 10132-4 Grade C67S Quenched Steel for High-Precision Cold-Rolled Strips
- EN 10132-4 Grade C75S – Quenched Cold-Rolled Steel for Springs & Precision Applications
- EN 10132-4 Grade C85S Quenched (+Q) Steel – Precision Cold-Rolled Strip for Springs