EN 10273 Grade 10CrMo9-10: Precision-Processed Steel Bars for High-Pressure Applications
Hot rolled weldable steel bars for pressure purposes with specified elevated temperature properties.
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 7.84 - 7.85 g/cm³ |
Mechanical
| Property | Temperature | Value |
|---|---|---|
Elastic modulus | -100.0 °C | 217 GPa |
20.0 °C | 212 - 212.43 GPa | |
100.0 °C | 207 - 207.49 GPa | |
200.0 °C | 199 - 201.15 GPa | |
300.0 °C | 192 - 193.89 GPa | |
400.0 °C | 184 - 185.24 GPa | |
500.0 °C | 174.89 - 175 GPa | |
600.0 °C | 163.15 - 164 GPa | |
Elongation | 20.0 °C | 17 % |
Poisson's ratio | 20.0 °C | 0.28 [-] |
100.0 °C | 0.29 [-] | |
200.0 °C | 0.29 [-] | |
300.0 °C | 0.29 [-] | |
400.0 °C | 0.3 [-] | |
500.0 °C | 0.31 [-] | |
600.0 °C | 0.31 [-] | |
Shear modulus | 20.0 °C | 82.81 GPa |
100.0 °C | 80.65 GPa | |
200.0 °C | 77.87 GPa | |
300.0 °C | 74.93 GPa | |
400.0 °C | 71.22 GPa | |
500.0 °C | 66.9 GPa | |
600.0 °C | 62.11 GPa | |
Tensile strength | 20.0 °C | 460 - 620 MPa |
Yield strength | 20.0 °C | 250 - 270 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | -100.0 °C | 1.05E-5 1/K | |
20.0 °C | 1.15E-5 1/K | ||
100.0 °C | 1.21E-5 1/K | ||
200.0 °C | 1.27E-5 1/K | ||
300.0 °C | 1.32E-5 1/K | ||
400.0 °C | 1.36E-5 1/K | ||
500.0 °C | 1.4E-5 1/K | ||
600.0 °C | 1.44E-5 1/K | ||
Melting point | 1382 - 1529 °C | Typical for Chromium Molybdenum Steel | |
Specific heat capacity | -100.0 °C | 423 J/(kg·K) | |
20.0 °C | 461 J/(kg·K) | ||
100.0 °C | 479 J/(kg·K) | ||
200.0 °C | 499 J/(kg·K) | ||
300.0 °C | 517 J/(kg·K) | ||
400.0 °C | 536 J/(kg·K) | ||
500.0 °C | 558 J/(kg·K) | ||
600.0 °C | 587 J/(kg·K) | ||
Thermal conductivity | 20.0 °C | 34.9 W/(m·K) | |
100.0 °C | 37.3 W/(m·K) | ||
200.0 °C | 38.2 W/(m·K) | ||
300.0 °C | 37.8 W/(m·K) | ||
400.0 °C | 36.6 W/(m·K) | ||
500.0 °C | 35.2 W/(m·K) | ||
600.0 °C | 33.6 W/(m·K) | ||
Thermal diffusivity | 20.0 °C | 9.7 mm²/s | |
100.0 °C | 9.6 mm²/s | ||
200.0 °C | 9.2 mm²/s | ||
300.0 °C | 8.5 mm²/s | ||
400.0 °C | 7.8 mm²/s | ||
500.0 °C | 6.8 mm²/s | ||
600.0 °C | 5.7 mm²/s | ||
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical resistivity | 20.0 °C | 2.98E-7 Ω·m |
100.0 °C | 3.43E-7 Ω·m | |
200.0 °C | 4.13E-7 Ω·m | |
300.0 °C | 4.97E-7 Ω·m | |
400.0 °C | 5.95E-7 Ω·m | |
500.0 °C | 7.03E-7 Ω·m | |
600.0 °C | 8.25E-7 Ω·m | |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.08 - 0.14 % |
Chromium | 2 - 2.5 % |
Copper | 0.3 % |
Manganese | 0.4 - 0.8 % |
Molybdenum | 0.9 - 1.1 % |
Nitrogen | 0.01 % |
Phosphorus | 0.02 % |
Silicon | 0.5 % |
Sulfur | 0.01 % |
Metal
- EN 10222-3 Grade 12Ni14 – High-Performance Nickel Alloy for Cryogenic Applications
- EN 10222-3 X8Ni9: High‑Performance Nickel Alloy for Cryogenic Applications
- EN 10273 13CrMo4-5 Quenched & Tempered Steel – High-Temperature Performance
- ASTM A727 Grade A727 – Normalized, Normalized & Tempered, or Quenched & Tempered Steel
- EN 10273 13CrMo4-5 Steel Bars – Normalized & Tempered or Quenched & Tempered for High-Pressure Applications
- EN 10222-3 Grade 15NiMn6: Normalized/Tempered or Quenched/Tempered Nickel Steel
- EN 10222-3 X12Ni5: High-Performance Normalized & Tempered Nickel Steel for Low-Temperature Forging
- EN 10273 10CrMo9-10 Steel – Normalized & Tempered (NT) for High‑Temperature Boiler Applications
- EN 10273 Grade 13CrMo4-5 – Normalized & Tempered High-Temperature Steel
- EN 10028-4 Grade X8Ni9: Cryogenic Ni-Alloy Steel (Normalized/Quenched & Tempered)