DIN 2391-2 St 30 Al Seamless Steel Tube – Soft Annealed, Grade A
Seamless precision steel tube made from St 30 Al is mainly used as construction element with special requirements in dimension accuracy, small wall thicknesses and good surface condition. The tubes are made in different grades (A and C). Grade C is valid for conduits. Grade A: for mechanical load without special grade requirement, without inspection certificate Grade C: for special requirements (testing after arrangement, e.g. bending, flanging, bulging a.o.) The weldability is given. Application (acc. VdTÜV-Wbl 445 : 2001-09): pressure vessels acc. TRB 100 and AD-Merkblatt W 4 from -10 to 300 degrees C, for steam boilers acc. TRD 702, for tube parts acc. TRbF 131 and 212 analogical St 37.0 in DIN 1629 as well as in the nuclear engineering.
Properties
General
| Property | Temperature | Value | Comment |
|---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa | Typical for Low Carbon Steel |
Elongation | 20.0 °C | 30 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] | Typical for Low Carbon Steel |
Shear modulus | 23.0 °C | 82 GPa | Typical for Low Carbon Steel |
Tensile strength | 20.0 °C | 280 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Max service temperature | 500 °C | Typical for Carbon Steel | |
Melting point | 1480 - 1526 °C | Typical for Low Carbon Steel | |
Specific heat capacity | 23.0 °C | 465 J/(kg·K) | Typical for Low Carbon Steel |
Thermal conductivity | 23.0 °C | 25 - 93 W/(m·K) | Typical for Low Carbon Steel |
Electrical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Electrical resistivity | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Magnetic
| Property | Value | Comment |
|---|---|---|
Curie temperature | 770 °C | Typical for Low Carbon Steel |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.1 % |
Manganese | 0.55 % |
Phosphorus | 0.03 % |
Silicon | 0.05 % |
Sulfur | 0.025 % |
Metal
- DIN 17442 X38CrMoV15 Soft-Annealed Stainless Steel – Superior Corrosion Resistance
- DIN 17210 Grade 21NiCrMo2 Soft Annealed Steel – Superior Wear Resistance & Fatigue Strength
- DIN 17210 Grade 20CrS4 Soft Annealed Steel: High Wear Resistance & Machinability
- DIN 17210 Grade 21NiCrMoS2 Soft Annealed Steel (+A) – High Performance for Wear-Resistant Applications
- DIN 17210 Grade 20Cr4 Soft‑Annealed Steel – High Wear Resistance for Automotive & Mechanical Applications
- DIN 17210 Grade 20MoCrS4 Soft Annealed Steel – Superior Wear Resistance & Fatigue Strength
- DIN 2391-2 St 30 Si Soft‑Annealed Tube – Grade A for Precision Construction
- DIN 2391-2 Grade St 45 Soft Annealed Steel Tube – Precision, Thin Walls, Superior Surface
- DIN 2391-2 St 52 Soft Annealed Steel Tube – Grade A – Precision Seamless Construction Element
- DIN 2391‑2 St 35 Soft Annealed Steel Tubes – Precision, Low Wall Thickness, Reliable Weldability