EN 573-3 Grade 3.3549 H19 – High-Performance Alloy with Superior Strength
Quantity: One truck load – Specialty products on request.Additional services: Via Cindal (the Aludium R&D department): R&D services, benchmarking, chemical audits, material specification, process optimisation, quality monitoring, sample analysis, prototyping, training
Properties
General
| Property | Value | Condition | Related Standards |
|---|---|---|---|
Density | 2.65 g/cm³ | H19 | EN 573-3, EN 485, EN 541 |
Mechanical
| Property | Value | Condition | Related Standards | Comment |
|---|---|---|---|---|
Elastic modulus | 70.0 GPa | H19 | EN 573-3, EN 485, EN 541 | |
Hardness, Brinell | 114.0 [-] | H19 | EN 573-3, EN 485 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||
Poisson's ratio | 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||
Shear modulus | 26.0 - 26.5 GPa | Typical for Wrought 5000 Series Aluminium | ||
Tensile strength | 370.0 - 430.0 MPa | H19 | EN 573-3, EN 541 | |
380.0 MPa | H19 | EN 573-3, EN 485 |
Thermal
| Property | Temperature | Value | Condition | Related Standards | Comment |
|---|---|---|---|---|---|
Coefficient of thermal expansion | 20 °C | 2.3199999999999998e-05 1/K | H19 | EN 573-3, EN 485, EN 541 | |
100 °C | 2.3199999999999998e-05 1/K | H19 | EN 573-3, EN 485, EN 541 | ||
Max service temperature | 150.0 °C | Typical for Wrought 5000 Series Aluminium | |||
Melting point | 577.0 - 638.0 °C | H19 | EN 573-3, EN 485, EN 541 | ||
Specific heat capacity | 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | |||
Thermal conductivity | 123 W/(m·K) | H19 | EN 573-3, EN 485, EN 541 |
Electrical
| Property | Value | Condition | Related Standards |
|---|---|---|---|
Electrical conductivity | 18000000.0 S/m | H19 | EN 573-3, EN 485, EN 541 |
Electrical resistivity | 5.56e-08 Ω·m | H19 | EN 573-3, EN 485, EN 541 |
Chemical properties
| Property | Value | Condition | Related Standards |
|---|---|---|---|
Chromium | 0.1 % | H19 | EN 573-3, EN 485, EN 541 |
Copper | 0.15 % | H19 | EN 573-3, EN 485, EN 541 |
Iron | 0.35 % | H19 | EN 573-3, EN 485, EN 541 |
Magnesium | 4.0 - 5.0 % | H19 | EN 573-3, EN 485, EN 541 |
Manganese | 0.2 - 0.5 % | H19 | EN 573-3, EN 485, EN 541 |
Silicon | 0.2 % | H19 | EN 573-3, EN 485, EN 541 |
Titanium | 0.1 % | H19 | EN 573-3, EN 485, EN 541 |
Zinc | 0.25 % | H19 | EN 573-3, EN 485, EN 541 |
Technological properties
| Property | ||
|---|---|---|
| Workability | Good workability. | |
Metal
- EN 573-3 Grade 3.3549 F – Premium Aluminum Alloy with Expert R&D Support
- EN 573-3 Grade 3.3549 H48 – Premium Aluminium Alloy for Structural Applications
- EN 573-3 Grade 3.0505 H19 – Premium Wrought Aluminum Alloy
- EN 573-3 Grade 3.0515 H19 Aluminium: Properties, Standards, and Applications
- EN 573-3 Grade 3.3315 H19 Aluminium – Specifications & Properties
- EN 573-3 Grade 3.0257 H19 Aluminium – Specifications & Performance
- EN 573-3 Grade 3.3206 H19 – High-Performance Aluminium Alloy
- EN 573-3 Grade 3.0525 H19 – Premium Aluminium Alloy Specification
- EN 573-3 Grade 3.0526 H19 Aluminium – Properties & Standards
- EN 573-3 Grade 3.3549 O – Premium Aluminum Alloy Supplier