EN 573-3 Grade 3.3315 H36: Key Mechanical Properties & Standards
Properties
General
| Property | Value | Condition | Related Standards |
|---|---|---|---|
Density | 2.69 g/cm³ | H36 | EN 573-3, EN 485 |
Mechanical
| Property | Value | Condition | Related Standards | Comment |
|---|---|---|---|---|
Bending angle 90° | 1.0 °/t | H36 | EN 573-3, EN 485 | |
1.5 °/t | H36 | EN 573-3, EN 485 | ||
2.0 °/t | H36 | EN 573-3, EN 485 | ||
2.5 °/t | H36 | EN 573-3, EN 485 | ||
Elastic modulus | 69.5 GPa | H36 | EN 573-3, EN 485 | |
Hardness, Brinell | 52.0 [-] | H36 | EN 573-3, EN 485 | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m | Typical for Wrought 5000 Series Aluminium | ||
Poisson's ratio | 0.33 [-] | Typical for Wrought 5000 Series Aluminium | ||
Shear modulus | 26.1 GPa | H36 | EN 573-3, EN 485 | |
Tensile strength | 165.0 - 205.0 MPa | H36 | EN 573-3, EN 485 |
Thermal
| Property | Temperature | Value | Condition | Related Standards | Comment |
|---|---|---|---|---|---|
Coefficient of thermal expansion | -50 °C | 2.18e-05 1/K | H36 | EN 573-3, EN 485 | |
20 °C | 2.18e-05 1/K | H36 | EN 573-3, EN 485 | ||
20 °C | 2.36e-05 1/K | H36 | EN 573-3, EN 485 | ||
20 °C | 2.45e-05 1/K | H36 | EN 573-3, EN 485 | ||
20 °C | 2.55e-05 1/K | H36 | EN 573-3, EN 485 | ||
100 °C | 2.36e-05 1/K | H36 | EN 573-3, EN 485 | ||
200 °C | 2.45e-05 1/K | H36 | EN 573-3, EN 485 | ||
300 °C | 2.55e-05 1/K | H36 | EN 573-3, EN 485 | ||
Max service temperature | 150.0 °C | Typical for Wrought 5000 Series Aluminium | |||
Melting point | 630.0 - 650.0 °C | H36 | EN 573-3, EN 485 | ||
Specific heat capacity | 879.0 - 963.0 J/(kg·K) | Typical for Wrought 5000 Series Aluminium | |||
Thermal conductivity | 160.0 - 220.0 W/(m·K) | H36 | EN 573-3, EN 485 |
Electrical
| Property | Value | Condition | Related Standards |
|---|---|---|---|
Electrical conductivity | 23000000.0 - 31000000.0 S/m | H36 | EN 573-3, EN 485 |
Electrical resistivity | 3.23e-08 - 4.35e-08 Ω·m | H36 | EN 573-3, EN 485 |
Chemical properties
| Property | Value | Condition | Related Standards |
|---|---|---|---|
Chromium | 0.1 % | H36 | EN 573-3, EN 485 |
Copper | 0.2 % | H36 | EN 573-3, EN 485 |
Iron | 0.70 % | H36 | EN 573-3, EN 485 |
Magnesium | 1.1 - 1.8 % | H36 | EN 573-3, EN 485 |
Manganese | 0.3 % | H36 | EN 573-3, EN 485 |
Silicon | 0.4 % | H36 | EN 573-3, EN 485 |
Zinc | 0.25 % | H36 | EN 573-3, EN 485 |
Technological properties
| Property | ||
|---|---|---|
| Workability | Good workability. | |
Metal
- AW-3005 H36 Aluminium Alloy – EN 573-3 Grade, High-Strength & Versatile
- EN 573-3 Grade 3.3315 H112 – Comprehensive Material Specifications
- EN 573-3 Grade 3.3315 H19 Aluminium – Specifications & Properties
- EN 573-3 Grade 3.0525 H36 Aluminium – Key Properties & Standards
- AW-3103 H36 Aluminium Alloy – EN 573-3 Certified
- EN 573-3 Grade 3.3315 (H26) – Standard Aluminum Alloy
- EN 573-3 Grade 3.3315 H38 – Aluminium Specification & Performance
- EN 573-3 Grade 3.3316 H36 – Steel Specifications & Standards
- EN 573-3 Grade 3.3315 H34 – Comprehensive Material Specifications
- EN 573-3 Grade 3.3315 H32: Key Mechanical Properties & Standards