Properties
General
| Property | Value | Condition | Related Standards | Shape |
|---|---|---|---|---|
Density | 2.72 g/cm³ | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Mechanical
| Property | Value | Condition | Related Standards | Shape | Comment |
|---|---|---|---|---|---|
Elastic modulus | 70.0 GPa | Typical for Wrought 6000 Series Aluminium | |||
Elongation | 4.0 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m | Typical for Wrought 6000 Series Aluminium | |||
Poisson's ratio | 0.33 [-] | Typical for Wrought 6000 Series Aluminium | |||
Shear modulus | 26.0 - 26.5 GPa | Typical for Wrought 6000 Series Aluminium | |||
Tensile strength | 160.0 - 240.0 MPa | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Thermal
| Property | Value | Comment |
|---|---|---|
Coefficient of thermal expansion | 1.6e-05 - 2.4e-05 1/K | Typical for Wrought 6000 Series Aluminium |
Melting point | 555.0 - 655.0 °C | Typical for Wrought 6000 Series Aluminium |
Specific heat capacity | 887.0 - 963.0 J/(kg·K) | Typical for Wrought 6000 Series Aluminium |
Thermal conductivity | 170.0 - 220.0 W/(m·K) | Typical for Wrought 6000 Series Aluminium |
Electrical
| Property | Value | Comment |
|---|---|---|
Electrical conductivity | 21000000.0 - 34000000.0 S/m | Typical for Wrought 6000 Series Aluminium |
Electrical resistivity | 2.9e-08 - 5e-08 Ω·m | Typical for Wrought 6000 Series Aluminium |
Chemical properties
| Property | Value | Condition | Related Standards | Shape |
|---|---|---|---|---|
Chromium | 0.25 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Copper | 0.5 - 1.1 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Iron | 0.5 % | H13 | EN 573-3 | |
0.50 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar | |
Magnesium | 0.6 - 1.2 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Manganese | 0.4 - 1.0 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Silicon | 0.7 - 1.3 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Zinc | 0.1 - 0.7 % | H13 | EN 573-3, EN 1301 | Strip, Sheet, Plate, Tube, Bar |
Technological properties
| Property | ||
|---|---|---|
| Workability | Excellent workability. | |
Metal
- AW-6056 F Aluminium Grade (EN 573-3) – Technical Specifications & Properties
- AW-6056 O3: EN 573-3 Grade Aluminium Properties & Standards
- EN 573-3 Grade 3.1305 H13 – High Strength Aluminium Alloy
- EN 573-3 Grade AW-1350 H13 Aluminium Alloy – Properties & Standards
- H13 Grade 3.2315 Steel – EN 573-3 Specification
- EN 573-3 Grade 3.1325 H13 – High-Strength Wrought Aluminium Alloy Specifications
- EN 573-3 Grade AW-6056 H18 – High-Strength Age-Hardenable AlMgSi Alloy
- EN 573-3 Grade AW-2011 H13 Aluminum Alloy – Superior Machining & Mechanical Performance
- AW-6056 T6 Aluminium Alloy – EN 573-3 Certified Grade
- EN 573-3 Grade AW-6056 T4 – High-Performance Age-Hardenable AlMgSi Alloy