EN 10139 Grade DC01 Cold-Rolled Steel – Skin-Passed, Ideal for Precision Cold Forming
Cold rolled uncoated low carbon steel narrow strip for cold forming.,The non-alloy steel DC01 acc. to DIN EN 10130 is suitable for cold forming of simple profile forms and components. Mechanical foldings are possible for thicknesses of up to 1,5 mm. To freedom of stretcher strains applies a period of 3 months after provision of the products for surface type B. Welding: DC01 is weldable by the following welding methods: MAG (metal-active-gas), plasma welding, laser welding, compression weld welding, resistance welding (spot, roll weld, buckle welding), arc welding. The steel acts as substrate for surface refined and coated bands and sheets. Application of DC01: household appliances industry, construction trade, car manufacturing, traffic system. Acc. to DIN EN 10139 DC01 is offered as cold rolled band or bar, cut in strength range HK270 to HK690. On welding of DC01in condition HK290 to HK690 has to be considered the potential influence to the mechanical properties
Properties
General
| Property | Temperature | Value | Comment |
|---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 20.0 °C | 200 - 215 GPa | Typical for Low Carbon Steel |
Elongation | 20.0 °C | 32 % | |
Elongation A50 | 20.0 °C | 22 - 30 % | |
Elongation A80 | 20.0 °C | 20 - 28 % | |
Hardness, Vickers | 20.0 °C | 115 - 125 [-] | |
Poisson's ratio | 20.0 °C | 0.29 [-] | Typical for Low Carbon Steel |
Tensile strength | 20.0 °C | 270 - 410 MPa | |
Yield strength | 20.0 °C | 140 - 320 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Melting point | 1480 - 1526 °C | Typical for Low Carbon Steel |
Magnetic
| Property | Value | Comment |
|---|---|---|
Curie temperature | 770 °C | Typical for Low Carbon Steel |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.12 % |
Manganese | 0.6 % |
Phosphorus | 0.05 % |
Sulfur | 0.045 % |
Metal
- EN 10139 Grade RRSt 3 – Cold‑Rolled, Skin‑Passed Steel for High‑Performance Tooling
- EN 10139 Grade St 2 Cold Rolled Steel – Skin-Passed, High Strength & Weldable
- EN 10139 St. 2 Cold‑Rolled, Skin‑Passed Steel (K32) – Superior Strength & Weldability
- EN 10139 Grade St 4 Cold-Rolled, Skin-Passed Steel (K32) – High Strength & Formability
- EN 10139 Grade USt 3: Cold‑Rolled, Skin‑Passed Steel for High‑Performance Applications
- EN 10139 DC05 Cold Rolled Low‑Carbon Steel – Skin Pass Grade
- EN 10139 Grade DC03: Cold Rolled, Skin-Passed Low-Carbon Steel Strip
- EN 10139 Grade DC04 Cold-Rolled Steel – High-Quality, Skin-Passed, Ideal for Cold Forming
- EN 10209 DC03ED: Cold-Rolled, Skin-Passed Low-Carbon Steel for Enamel Applications
- EN 10139 Grade DC06 Cold Rolled Low-Carbon Steel – Skin Passed