EN 10209 DC03ED: Cold-Rolled, Skin-Passed Low-Carbon Steel for Enamel Applications

Cold rolled low carbon steel for flat products for vitreous enamelling (direct enamelling, as well as for special applications of conventional two coat enamelling for better sag resistance). Application: domestic appliances (cooking, laundry), sanitary ware (bathtubs, shower trays, sinks), architectural panels (interior and exterior), signage,The soft unalloyed steel DCO1ED, mat. No. 1.0399, is a cold formable steel and suitable for direct enameling as well as for special conventional applications of two-coat enameling, especially if there should be preferably enameled non deforming. In this case are necessary special measures in order to improve enamel`s adhesion. Mechanical specific values and freedom of stretcher strains are warranted for 6 months. Application: simple reforming parts pots, pans, covering caps for gas kitchen stoves, baking sheets, simple shower bases etc. Welding: DC01ED is weldable acc. to the fusion welding methods: MAG (metal active gas/plasma welding arc hand welding laser welding gas welding resistance welding (spot, roll seam, buckle welding)

Properties

General

PropertyTemperatureValueComment

Density

20.0 °C

7.8 - 7.9 g/cm³

Typical for Low Carbon Steel

Mechanical

PropertyTemperatureValueComment

Elastic modulus

20.0 °C

200 - 215 GPa

Typical for Low Carbon Steel

Elongation A80

20.0 °C

34 %

Elongation A80, transverse

20.0 °C

30 - 34 %

Poisson's ratio

20.0 °C

0.29 [-]

Typical for Low Carbon Steel

Tensile strength

20.0 °C

270 - 370 MPa

Tensile strength, transverse

20.0 °C

270 - 370 MPa

Yield strength

20.0 °C

140 - 240 MPa

Yield strength, transverse

20.0 °C

140 - 280 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

1.32E-5 - 1.38E-5 1/K

Typical for Low Carbon Steel

Melting point

1480 - 1526 °C

Typical for Low Carbon Steel

Magnetic

PropertyValueComment

Curie temperature

770 °C

Typical for Low Carbon Steel

Chemical properties

PropertyValue

Carbon

4E-3 %

Manganese

0.4 %

Phosphorus

0.04 %

Sulfur

0.05 %


Metal

  1. EN 10139 Grade RRSt 3 – Cold‑Rolled, Skin‑Passed Steel for High‑Performance Tooling
  2. EN 10139 Grade St 2 Cold Rolled Steel – Skin-Passed, High Strength & Weldable
  3. EN 10139 St. 2 Cold‑Rolled, Skin‑Passed Steel (K32) – Superior Strength & Weldability
  4. EN 10139 Grade St 4 Cold-Rolled, Skin-Passed Steel (K32) – High Strength & Formability
  5. EN 10139 Grade USt 3: Cold‑Rolled, Skin‑Passed Steel for High‑Performance Applications
  6. EN 10139 DC05 Cold Rolled Low‑Carbon Steel – Skin Pass Grade
  7. EN 10139 Grade DC01 Cold-Rolled Steel – Skin-Passed, Ideal for Precision Cold Forming
  8. EN 10139 Grade DC03: Cold Rolled, Skin-Passed Low-Carbon Steel Strip
  9. EN 10139 Grade DC04 Cold-Rolled Steel – High-Quality, Skin-Passed, Ideal for Cold Forming
  10. EN 10139 Grade DC06 Cold Rolled Low-Carbon Steel – Skin Passed