EN 12451 Grade Cu-DHP H075 – Premium Copper Tubing for Heat Exchangers & Desalination

The material according this standard is used for seamless, round tubes for heat exchangers, condensers, evaporators and desalination equipment.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.9 - 8.94 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

-253.0 °C

138 GPa

-195.0 °C

136 GPa

-100.0 °C

133 GPa

20.0 °C

128 - 132 GPa

50.0 °C

127 GPa

100.0 °C

125 GPa

150.0 °C

122 GPa

200.0 °C

120 GPa

250.0 °C

118 GPa

Hardness, Brinell

20.0 °C

75 - 100 [-]

Hardness, Vickers

20.0 °C

75 - 105 [-]

Poisson's ratio

20.0 °C

0.34 [-]

Shear modulus

23.0 °C

48 GPa

Typical for Wrought Copper Pure / Low Alloyed Copper

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

1.68E-5 1/K

200.0 °C

1.73E-5 1/K

300.0 °C

1.77E-5 1/K

Melting point

965 - 1100 °C

Typical for Wrought Copper Pure / Low Alloyed Copper

Specific heat capacity

-150.0 °C

282 J/(kg·K)

-50.0 °C

361 J/(kg·K)

20.0 °C

386 J/(kg·K)

100.0 °C

393 J/(kg·K)

200.0 °C

403 J/(kg·K)

300.0 °C

415 J/(kg·K)

Thermal conductivity

20.0 °C

305 - 340 W/(m·K)

50.0 °C

310 W/(m·K)

100.0 °C

318 W/(m·K)

200.0 °C

326 W/(m·K)

300.0 °C

334 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

4.30E+7 S/m

50.0 °C

4.10E+7 S/m

100.0 °C

3.70E+7 S/m

200.0 °C

3.40E+7 S/m

300.0 °C

3.00E+7 S/m

Electrical resistivity

20.0 °C

2.2E-8 Ω·m

50.0 °C

2.4E-8 Ω·m

100.0 °C

2.7E-8 Ω·m

200.0 °C

2.9E-8 Ω·m

300.0 °C

3.3E-8 Ω·m

Chemical properties

PropertyValue

Copper

99.9 %

Phosphorus

0.02 - 0.04 %

Silver

0.02 %


Metal

  1. EN 1652 CuZn5 H075 – High‑Strength, Corrosion‑Resistant Wrought Alloy
  2. EN 13148 Cu-DHP H110: High-Quality Hot-Dip Tinned Copper Strip
  3. EN 12451 Cu-DHP H100 Seamless Tubing for High-Performance Heat Exchangers
  4. EN 12163 Grade Cu-DHP H075: High-Purity Phosphoric Copper for Superior Performance
  5. EN 12451 CuZn28Sn1As R320 Alloy – Ideal for Heat Exchangers & Desalination Tubes
  6. EN 12451 CuZn28Sn1As R360: Premium Copper Alloy for High-Performance Heat Exchangers
  7. EN 12451 CuZn30As O60 – Copper Brass Seamless Tube Grade
  8. EN 13148 Grade Cu-DHP R360 – Premium Hot-Dip Tinned Copper Strip
  9. EN 14436 Cu-DHP R290: Premium Copper for Electrolytically Tinned Strips
  10. EN 12166 Grade CuZn40Pb2 H075 – High‑Strength Lead‑Enhanced Copper Alloy