EN 10277‑2 Grade ZSt50‑2: Cold‑Drawn & Turned High‑Strength Steel
ZSt 50-2 is a bright drawn steel grade for wear and strength loaded parts (bolts, shafts, spindles).
Properties
General
| Property | Temperature | Value | Comment |
|---|---|---|---|
Density | 23.0 °C | 7.8 - 7.9 g/cm³ | Typical for Medium Carbon Steel |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 23.0 °C | 200 - 215 GPa | Typical for Medium Carbon Steel |
Elongation | 20.0 °C | 18 - 20 % | |
Poisson's ratio | 23.0 °C | 0.29 [-] | Typical for Medium Carbon Steel |
Shear modulus | 23.0 °C | 75 - 80 GPa | Typical for Carbon Steel |
Tensile strength | 20.0 °C | 470 - 610 MPa | |
Yield strength | 20.0 °C | 265 - 295 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.32E-5 1/K | Typical for Medium Carbon Steel |
Max service temperature | 500 °C | Typical for Carbon Steel | |
Melting point | 1380 - 1514 °C | Typical for Medium Carbon Steel | |
Specific heat capacity | 23.0 °C | 470 - 520 J/(kg·K) | Typical for Medium Carbon Steel |
Thermal conductivity | 23.0 °C | 21 - 52 W/(m·K) | Typical for Medium Carbon Steel |
Electrical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Electrical resistivity | 23.0 °C | 1.43E-7 - 1.74E-7 Ω·m | Typical for Carbon Steel |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.3 % |
Phosphorus | 0.05 % |
Sulfur | 0.05 % |
Metal
- EN 10277-2 Grade ZSt60-2: Cold‑Drawn, Turned & Normalized Steel for High‑Strength Applications
- EN 10277-2 Grade ZSt70-2: High-Performance Cold-Drawn & Normalized Steel for Wear-Resistant Applications
- EN 10277-2 Grade St 50-2: Premium Cold‑Drawn Structural Steel for High‑Performance Applications
- EN 10277-2 Grade St 60-2 – Premium Cold‑Drawn, Turned, and Normalized Structural Steel
- EN 10277-2 Grade St 70-2 – Cold Drawn or Turned, Normalized Structural Steel
- EN 10277-2 Grade St 37-2: Cold Drawn, Turned & Normalized Low‑Carbon Steel
- EN 10277-2 Grade ZSt52-3: Cold-Drawn, Turned, and Normalized High-Strength Structural Steel
- EN 10277-2 Grade St 44-3: Fine-Grained Cold-Drawn or Turned and Normalized Steel
- EN 10277-2: Grade St52-3 – Cold Drawn or Turned and Normalized Steel for High-Dynamic Load Applications
- EN 10277-2: Grade St 37‑3 – Cold Drawn/Turned & Normalized Structural Steel