EN 12166 CuSn6 H02 Alloy – Specifications & Applications

CuSn6, mat. No. CW425K, is comparable to the DIN-make CuSn6, mat. No. 2.1020, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Appliction: For all types of springs, especially in electrical industry, for connectors, hose and spring tubes, fabric and screening wires, gong bars. Further application in paper, cellulose and chemical industry, in shipbuilding and machine engineering. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.82 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 - 130 GPa

Typical for Leaded Phosphor Bronze

Elongation A10

20.0 °C

12 %

Elongation A100

20.0 °C

5 - 8 %

Hardness, Vickers

20.0 °C

160 - 195 [-]

Poisson's ratio

23.0 °C

0.33 [-]

Typical for Leaded Phosphor Bronze

Tensile strength

20.0 °C

510 - 710 MPa

Yield strength Rp0.2

20.0 °C

390 - 460 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.8E-5 1/K

200.0 °C

1.85E-5 1/K

650.0 °C

2.22E-5 1/K

800.0 °C

2.18E-5 1/K

Max service temperature, long

0 - 150 °C

Specific heat capacity

20.0 °C

377 J/(kg·K)

Thermal conductivity

20.0 °C

75 W/(m·K)

200.0 °C

98 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

9.00E+6 S/m

200.0 °C

7.80E+6 S/m

Electrical resistivity

20.0 °C

1.11E-7 Ω·m

200.0 °C

1.28E-7 Ω·m

Chemical properties

PropertyValue

Iron

0.1 %

Lead

0.02 %

Nickel

0.2 %

Phosphorus

0.01 - 0.4 %

Tin

5.5 - 7 %

Zinc

0.2 %


Metal

  1. EN 12166 Grade CuNi10Zn42Pb2 H02 – High-Performance Copper‑Nickel Alloy for Industrial Applications
  2. EN 12166 Grade CuNi12Zn30Pb1 – High Strength, Corrosion-Resistant Copper-Nickel-Zinc Alloy
  3. EN 12166 CuNi18Zn19Pb1 H02: High-Strength, Corrosion-Resistant Copper Alloy
  4. EN 12166 Grade CuSn6 H190 – Superior Tin‑Copper Alloy for Industrial Use
  5. EN 12166 Grade CuSn6 H245 – High-Performance Tin‑Copper Alloy for Corrosion Resistance
  6. EN 12166 Grade CuZn38Pb2 H02 – Standard Copper Brass Specifications
  7. EN 12166 CuZn37 (CW508L) – High-Strength, Corrosion-Resistant Copper Alloy for Cold Forming
  8. CuZn36 (CW507L) – Grade EN 12166: High-Strength, Machinable Copper Alloy
  9. EN 12166 CuSn6 R900: Premium Tin‑Copper Alloy for Superior Corrosion Resistance
  10. EN 12166 Grade CuSn6 H150 Copper Alloy Profile – High Strength & Excellent Thermal Performance