CuSn6, mat. No. CW425K, is comparable to the DIN-make CuSn6, mat. No. 2.1020, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Appliction: For all types of springs, especially in electrical industry, for connectors, hose and spring tubes, fabric and screening wires, gong bars. Further application in paper, cellulose and chemical industry, in shipbuilding and machine engineering. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 - 8.82 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

118 GPa

Poisson's ratio

20.0 °C

0.34 [-]

Tensile strength

20.0 °C

900 MPa

Yield strength Rp0.2

20.0 °C

800 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

1.8E-5 1/K

200.0 °C

1.85E-5 1/K

650.0 °C

2.22E-5 1/K

800.0 °C

2.18E-5 1/K

Max service temperature, long

0 - 150 °C

Specific heat capacity

20.0 °C

377 J/(kg·K)

Thermal conductivity

20.0 °C

75 W/(m·K)

200.0 °C

98 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

20.0 °C

9.00E+6 S/m

200.0 °C

7.80E+6 S/m

Electrical resistivity

20.0 °C

1.11E-7 Ω·m

200.0 °C

1.28E-7 Ω·m

Specific Electrical conductivity

16 % IACS

Chemical properties

PropertyValue

Iron

0.1 %

Lead

0.02 %

Nickel

0.2 %

Phosphorus

0.01 - 0.4 %

Tin

5.5 - 7 %

Zinc

0.2 %


Metal

  1. EN 12166 Grade CuSn6 H190 – Superior Tin‑Copper Alloy for Industrial Use
  2. EN 12166 Grade CuSn6 H245 – High-Performance Tin‑Copper Alloy for Corrosion Resistance
  3. EN 12166 Grade CuSn6 H150 Copper Alloy Profile – High Strength & Excellent Thermal Performance
  4. EN 12166 Grade CuSn6 H08 – High-Performance Copper Tin Alloy
  5. EN 12166 CuSn6 H04 – Premium Copper‑Tin Alloy for High Corrosion Resistance and Superior Mechanical Performance
  6. EN 12166 CuSn6 H03 – Premium Tin‑Copper Alloy for Corrosion Resistance
  7. EN 12166 Grade CuSn6 R700 – High-Performance Tin‑Copper Alloy
  8. EN 12166 CuSn6 H02 Alloy – Specifications & Applications
  9. EN 12166 Grade CuSn6 R520 – High‑Performance Tin‑Copper Alloy
  10. EN 12166 Grade CuSn6 H01 – Premium Tin‑Copper Alloy for Corrosion‑Resistant Applications