EN 12166 CuSn6 H04 – Premium Copper‑Tin Alloy for High Corrosion Resistance and Superior Mechanical Performance
CuSn6, mat. No. CW425K, is comparable to the DIN-make CuSn6, mat. No. 2.1020, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Appliction: For all types of springs, especially in electrical industry, for connectors, hose and spring tubes, fabric and screening wires, gong bars. Further application in paper, cellulose and chemical industry, in shipbuilding and machine engineering. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.82 g/cm³ |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Hardness, Vickers | 20.0 °C | 215 - 250 [-] | |
Poisson's ratio | 23.0 °C | 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 20.0 °C | 740 - 980 MPa | |
Yield strength Rp0.2 | 20.0 °C | 730 - 810 MPa |
Thermal
| Property | Temperature | Value |
|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.8E-5 1/K |
200.0 °C | 1.85E-5 1/K | |
650.0 °C | 2.22E-5 1/K | |
800.0 °C | 2.18E-5 1/K | |
Max service temperature, long | 0 - 150 °C | |
Specific heat capacity | 20.0 °C | 377 J/(kg·K) |
Thermal conductivity | 20.0 °C | 75 W/(m·K) |
200.0 °C | 98 W/(m·K) | |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 9.00E+6 S/m |
200.0 °C | 7.80E+6 S/m | |
Electrical resistivity | 20.0 °C | 1.11E-7 Ω·m |
200.0 °C | 1.28E-7 Ω·m | |
Chemical properties
| Property | Value |
|---|---|
Iron | 0.1 % |
Lead | 0.02 % |
Nickel | 0.2 % |
Phosphorus | 0.01 - 0.4 % |
Tin | 5.5 - 7 % |
Zinc | 0.2 % |
Metal
- EN 12166 CuNi10Zn42Pb2 H04 – High-Performance Wrought Copper Alloy
- EN 12166 Grade CuNi18Zn19Pb1 H04: High-Strength, Corrosion-Resistant Copper‑Nickel‑Zinc Alloy
- EN 12166 CuSn5 H04 – Premium Copper‑Tin Alloy for Precision Tubes and Connectors
- EN 12166 Grade CuSn6 H190 – Superior Tin‑Copper Alloy for Industrial Use
- EN 12166 Grade CuSn6 H245 – High-Performance Tin‑Copper Alloy for Corrosion Resistance
- EN 12166 Grade CuZn37 H04 – Premium Copper Alloy for Cold Forming & Corrosion Resistance
- EN 12166 CuZn36 H04 – Unhardenable Wrought Alloy for Precision Deep‑Drawing and Pressure Components
- EN 12166 CuSn6 R900: Premium Tin‑Copper Alloy for Superior Corrosion Resistance
- EN 12166 Grade CuSn6 H150 Copper Alloy Profile – High Strength & Excellent Thermal Performance
- EN 12166 Grade CuSn6 H08 – High-Performance Copper Tin Alloy