EN 12166 Grade CuSn6 H150 Copper Alloy Profile – High Strength & Excellent Thermal Performance
Copper alloy profiles and bars for general purposes.
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.8 - 8.82 g/cm³ |
Mechanical
| Property | Temperature | Value |
|---|---|---|
Elastic modulus | 20.0 °C | 118 GPa |
Hardness, Brinell | 20.0 °C | 150 - 180 [-] |
Hardness, Vickers | 20.0 °C | 155 [-] |
Poisson's ratio | 20.0 °C | 0.34 [-] |
Thermal
| Property | Temperature | Value |
|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.8E-5 1/K |
200.0 °C | 1.85E-5 1/K | |
650.0 °C | 2.22E-5 1/K | |
800.0 °C | 2.18E-5 1/K | |
Max service temperature, long | 0 - 150 °C | |
Specific heat capacity | 20.0 °C | 377 J/(kg·K) |
Thermal conductivity | 20.0 °C | 75 W/(m·K) |
200.0 °C | 98 W/(m·K) | |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 9.00E+6 S/m |
200.0 °C | 7.80E+6 S/m | |
Electrical resistivity | 20.0 °C | 1.11E-7 Ω·m |
200.0 °C | 1.28E-7 Ω·m | |
Specific Electrical conductivity | 16 % IACS | |
Chemical properties
| Property | Value |
|---|---|
Iron | 0.1 % |
Lead | 0.02 % |
Nickel | 0.2 % |
Phosphorus | 0.01 - 0.4 % |
Tin | 5.5 - 7 % |
Zinc | 0.2 % |
Metal
- EN 12166 Grade CuNi18Zn19Pb1 H150 – High-Strength, Corrosion-Resistant Alloy
- EN 12166 Grade CuSn6 H190 – Superior Tin‑Copper Alloy for Industrial Use
- EN 12166 Grade CuSn6 H245 – High-Performance Tin‑Copper Alloy for Corrosion Resistance
- EN 12166 CuSn6 R900: Premium Tin‑Copper Alloy for Superior Corrosion Resistance
- EN 12166 Grade CuSn6 H08 – High-Performance Copper Tin Alloy
- EN 12166 CuSn6 H04 – Premium Copper‑Tin Alloy for High Corrosion Resistance and Superior Mechanical Performance
- EN 12166 CuSn6 H03 – Premium Tin‑Copper Alloy for Corrosion Resistance
- EN 12166 Grade CuSn6 R700 – High-Performance Tin‑Copper Alloy
- EN 12166 CuSn6 H02 Alloy – Specifications & Applications
- EN 12166 Grade CuSn6 R520 – High‑Performance Tin‑Copper Alloy