EN 12166 Grade CuSn6 H08 – High-Performance Copper Tin Alloy
CuSn6, mat. No. CW425K, is comparable to the DIN-make CuSn6, mat. No. 2.1020, acc. to DIN 17662 : 1983-12. Properties of the CuSn-alloy are predominantly determined by the tin-content. Tensile strength, yield point and hardness increase according to the rising cold forming grade, elongation after fracture decreases. Electrical and thermal conductivity are lower than for pure copper. Very high resistance to corrosion, particularly to atmospheric influences, seawater, sulfite liquor, carbonated and salted mine water. The alloys are stress corrosion-proof. Processing properties: warm forming: medium cold forming: very good machinability: medium hard soldering: good soft soldering: good gas shielded welding: good burnishing: good Appliction: For all types of springs, especially in electrical industry, for connectors, hose and spring tubes, fabric and screening wires, gong bars. Further application in paper, cellulose and chemical industry, in shipbuilding and machine engineering. For the electrolytically tinned strip the coatings (Sn bright, Sn matt, Sn fuzed, SnPb) are listed by the application (better solderability, better corrosion resistance, reduction of the electrical contact resistance, better appearance) in the DIN EN 14436 : 2004-11 (Table 5)
Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 8.82 g/cm³ |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Hardness, Vickers | 20.0 °C | 245 [-] | |
Poisson's ratio | 23.0 °C | 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 20.0 °C | 900 - 980 MPa | |
Yield strength Rp0.2 | 20.0 °C | 890 - 960 MPa |
Thermal
| Property | Temperature | Value |
|---|---|---|
Coefficient of thermal expansion | 100.0 °C | 1.8E-5 1/K |
200.0 °C | 1.85E-5 1/K | |
650.0 °C | 2.22E-5 1/K | |
800.0 °C | 2.18E-5 1/K | |
Max service temperature, long | 0 - 150 °C | |
Specific heat capacity | 20.0 °C | 377 J/(kg·K) |
Thermal conductivity | 20.0 °C | 75 W/(m·K) |
200.0 °C | 98 W/(m·K) | |
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical conductivity | 20.0 °C | 9.00E+6 S/m |
200.0 °C | 7.80E+6 S/m | |
Electrical resistivity | 20.0 °C | 1.11E-7 Ω·m |
200.0 °C | 1.28E-7 Ω·m | |
Chemical properties
| Property | Value |
|---|---|
Iron | 0.1 % |
Lead | 0.02 % |
Nickel | 0.2 % |
Phosphorus | 0.01 - 0.4 % |
Tin | 5.5 - 7 % |
Zinc | 0.2 % |
Metal
- EN 12166 Grade CuSn5 H08 – Premium CuSn5 Tubes & Springs for Precision Engineering
- EN 12166 Grade CuSn6 H190 – Superior Tin‑Copper Alloy for Industrial Use
- EN 12166 Grade CuSn6 H245 – High-Performance Tin‑Copper Alloy for Corrosion Resistance
- EN 12166: CuZn37 (H08) – High‑Performance Copper Alloy for Cold Forming and Corrosion Resistance
- EN 12166 CuZn36 (CW507L) – High-Strength, Unhardenable Wrought Copper Alloy
- EN 12166 CuSn6 R900: Premium Tin‑Copper Alloy for Superior Corrosion Resistance
- EN 12166 Grade CuSn6 H150 Copper Alloy Profile – High Strength & Excellent Thermal Performance
- EN 12166 CuSn6 H04 – Premium Copper‑Tin Alloy for High Corrosion Resistance and Superior Mechanical Performance
- EN 12166 Grade CuZn40Pb2 H08: Unhardenable Wrought Alloy with Enhanced Machinability
- EN 12166 Grade CuZn39Pb3 H08 – Lead-Added Brass for Enhanced Machinability and Corrosion Resistance