EN 10139 Grade DC04 Cold‑Rolled, Strain‑Hardened Steel (C290) – High‑Performance Cold Forming Strip
Cold rolled uncoated low carbon steel narrow strip for cold forming.,The non-alloy steel DC04 acc. to DIN EN 10130 is as a deep-draw quality suitable for cold forming of complexest profile forms and components, especially at high deformation speeds (e.g. transfer presses). To freedom of stretcher strains applies a period of 6 months after provision of the products for surface type A and B. Welding: DC04 is weldable by the following welding methods: MAG (metal-active-gas), plasma welding, laser welding, compression weld welding, resistance welding (spot, roll weld, buckle welding), arc welding. The steel acts as substrate for surface refined and coated bands and sheets. Application of DC04: household appliances industry, construction trade. Acc. to DIN EN 10139 DC04 is offered as cold rolled band or bar, cut in strength range HK270 to HK590. On welding of DC04 in condition HK290 to HK590 has to be considered the potential influence to the mechanical properties
Properties
General
| Property | Temperature | Value | Comment |
|---|---|---|---|
Density | 20.0 °C | 7.8 - 7.9 g/cm³ | Typical for Low Carbon Steel |
Mechanical
| Property | Temperature | Value | Comment |
|---|---|---|---|
Elastic modulus | 20.0 °C | 200 - 215 GPa | Typical for Low Carbon Steel |
Elongation | 20.0 °C | 28 % | |
Elongation A50 | 20.0 °C | 26 % | |
Elongation A80 | 20.0 °C | 24 % | |
Hardness, Vickers | 20.0 °C | 95 - 117 [-] | |
Poisson's ratio | 20.0 °C | 0.29 [-] | Typical for Low Carbon Steel |
Tensile strength | 20.0 °C | 290 - 390 MPa | |
Yield strength | 20.0 °C | 220 - 325 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | 20.0 °C | 1.32E-5 - 1.38E-5 1/K | Typical for Low Carbon Steel |
Melting point | 1480 - 1526 °C | Typical for Low Carbon Steel |
Magnetic
| Property | Value | Comment |
|---|---|---|
Curie temperature | 770 °C | Typical for Low Carbon Steel |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.08 % |
Manganese | 0.4 % |
Phosphorus | 0.03 - 0.04 % |
Sulfur | 0.03 - 0.035 % |
Metal
- EN 10139 DC05 Cold Rolled Low‑Carbon Steel – Skin Pass Grade
- EN 10139 Grade DC01 Cold-Rolled Steel – Skin-Passed, Ideal for Precision Cold Forming
- EN 10139 Grade DC03: Cold Rolled, Skin-Passed Low-Carbon Steel Strip
- EN 10139 Grade DC04 Cold-Rolled Steel – High-Quality, Skin-Passed, Ideal for Cold Forming
- EN 10139 Grade DC04 Cold Rolled, Annealed Steel – Ideal for High‑Speed Cold Forming
- EN 10139 DC01 Cold-Rolled, Strain-Hardened Steel – Grade C290 – Ideal for Cold Forming
- EN 10139 Grade DC03: Cold-Rolled, Strain-Hardened Low-Carbon Steel (C290) for Precision Cold Forming
- EN 10139 Grade DC04 Cold‑Rolled, Strain‑Hardened Steel (C290) – High‑Performance Cold Forming Strip
- EN 10139 Grade DC04 Soft Annealed Steel Strip (+A) – Ideal for Cold Forming
- EN 10139 DC01 Grade Steel – C290 Work‑Hardened for Automotive & Industrial Applications