EN 10028-7 Grade X5CrNi18-10 Solution Annealed (+AT) – High-Performance Austenitic Stainless Steel
The basic type of the austenitic CrNi-steels X5CrNi18-10 shows high corrosion resistance but no resistance to intercrystalline corrosion in sensitized condition as well as favorable workability. The steel is suitable for mirror-polishing, is well cold formable, weldable and wear resistant. Application for welded parts in chemical apparatus engineering, food and milk industry, for household appliances, in breweries, in architecture and vehicle manufacturing as well as for pumps, compressors, instruments. Application also in water and low contaminated sewages. In pressure vessel construction up to 300 °C, above subject to authorization. The sort is acc. to DIN EN 10095 allowed to be used as a heat-resistant steel. Application temperature: -200 to 550 °C. In construction trade X5CrNi18-10 is applicated for decorative purposes in exterior and interior architecture, e.g. roof and wall elements, facings, washing plants, washbasins in toilets, for doors and windows. The material is approved for structural components (extended approval certificate Nr. Z-30.44.1 of Institut für Bautechnik Berlin, dated 01/02/89, containing demands for materials, calculation, construction and control). Strength grades E 225 and E 355 are common.
Additional services: To ensure our customers' processes and/or products attain – and even exceed – their performance expectations, we offer a wide range of services within both the technical area and delivery logistics. Our technical services include: • Material consultations through our worldwide sales network • Advice in process optimization based on an in-depth applications knowledge • Joint new product development supported by our extensive R&D program View product groups and servicesUGITECH
MANUFACTURER
Information and services
Additional services: https://eservices.ugitech.com/Properties
General
| Property | Temperature | Value |
|---|---|---|
Density | 20.0 °C | 7.9 - 7.92 g/cm³ |
Mechanical
| Property | Temperature | Value |
|---|---|---|
Elastic modulus | -100.0 °C | 206 GPa |
20.0 °C | 196 - 200 GPa | |
24.0 °C | 194.4 - 196.5 GPa | |
100.0 °C | 190 - 194 GPa | |
149.0 °C | 188.2 - 189.6 GPa | |
200.0 °C | 182 - 186 GPa | |
260.0 °C | 182.7 - 184.1 GPa | |
300.0 °C | 174 - 179 GPa | |
371.0 °C | 173.1 - 177.9 GPa | |
400.0 °C | 166 - 172 GPa | |
483.0 °C | 157.9 - 160 GPa | |
500.0 °C | 158 - 165 GPa | |
593.0 °C | 149.6 - 155.8 GPa | |
600.0 °C | 150 GPa | |
700.0 °C | 142 GPa | |
704.0 °C | 137.9 - 144.8 GPa | |
800.0 °C | 134 GPa | |
816.0 °C | 120.7 - 128.2 GPa | |
Elongation | -196.0 °C | 30 % |
-150.0 °C | 30 % | |
-80.0 °C | 35 % | |
20.0 °C | 45 % | |
Elongation A80, transverse | 20.0 °C | 45 % |
Elongation, transverse | 20.0 °C | 45 % |
Poisson's ratio | 20.0 °C | 0.28 [-] |
24.0 °C | 0.24 - 0.25 [-] | |
149.0 °C | 0.27 - 0.3 [-] | |
260.0 °C | 0.29 - 0.32 [-] | |
371.0 °C | 0.32 [-] | |
483.0 °C | 0.27 - 0.29 [-] | |
593.0 °C | 0.29 - 0.3 [-] | |
704.0 °C | 0.27 - 0.3 [-] | |
816.0 °C | 0.23 - 0.27 [-] | |
Shear modulus | 24.0 °C | 78.6 GPa |
149.0 °C | 72.4 - 74.5 GPa | |
260.0 °C | 69.6 - 71 GPa | |
371.0 °C | 65.5 - 67.6 GPa | |
483.0 °C | 62.1 GPa | |
593.0 °C | 57.9 - 60 GPa | |
704.0 °C | 54.5 - 55.9 GPa | |
816.0 °C | 49 - 50.3 GPa | |
Tensile strength | -196.0 °C | 1250 MPa |
-150.0 °C | 1100 MPa | |
-80.0 °C | 860 MPa | |
20.0 °C | 520 - 750 MPa | |
50.0 °C | 494 MPa | |
100.0 °C | 450 MPa | |
150.0 °C | 420 MPa | |
200.0 °C | 400 MPa | |
250.0 °C | 390 MPa | |
300.0 °C | 380 MPa | |
350.0 °C | 380 MPa | |
400.0 °C | 380 MPa | |
450.0 °C | 370 MPa | |
500.0 °C | 360 MPa | |
550.0 °C | 330 MPa | |
Tensile strength, transverse | 20.0 °C | 520 - 750 MPa |
Yield strength Rp0.2 | -196.0 °C | 300 MPa |
-150.0 °C | 315 MPa | |
-80.0 °C | 270 MPa | |
20.0 °C | 210 MPa | |
50.0 °C | 190 MPa | |
100.0 °C | 157 MPa | |
150.0 °C | 142 MPa | |
200.0 °C | 127 MPa | |
250.0 °C | 118 MPa | |
300.0 °C | 110 MPa | |
350.0 °C | 104 MPa | |
400.0 °C | 98 MPa | |
450.0 °C | 95 MPa | |
500.0 °C | 92 MPa | |
550.0 °C | 90 MPa | |
Yield strength Rp0.2, transverse | 20.0 °C | 210 - 230 MPa |
Yield strength Rp1.0 | -196.0 °C | 400 MPa |
-150.0 °C | 415 MPa | |
-80.0 °C | 350 MPa | |
20.0 °C | 250 MPa | |
50.0 °C | 228 MPa | |
100.0 °C | 191 MPa | |
150.0 °C | 172 MPa | |
200.0 °C | 157 MPa | |
250.0 °C | 145 MPa | |
300.0 °C | 135 MPa | |
350.0 °C | 129 MPa | |
400.0 °C | 125 MPa | |
450.0 °C | 122 MPa | |
500.0 °C | 120 MPa | |
550.0 °C | 120 MPa | |
Yield strength Rp1.0, transverse | 20.0 °C | 250 - 260 MPa |
Thermal
| Property | Temperature | Value | Comment |
|---|---|---|---|
Coefficient of thermal expansion | -100.0 °C | 1.49E-5 1/K | |
20.0 °C | 1.61E-5 1/K | ||
100.0 °C | 1.6E-5 - 1.67E-5 1/K | ||
200.0 °C | 1.65E-5 - 1.72E-5 1/K | ||
300.0 °C | 1.7E-5 - 1.77E-5 1/K | ||
400.0 °C | 1.75E-5 - 1.81E-5 1/K | ||
500.0 °C | 1.8E-5 - 1.84E-5 1/K | ||
600.0 °C | 1.88E-5 1/K | ||
700.0 °C | 1.91E-5 1/K | ||
800.0 °C | 1.94E-5 1/K | ||
Max service temperature, long | -200 - 550 °C | ||
Melting point | 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Specific heat capacity | -100.0 °C | 440 J/(kg·K) | |
20.0 °C | 472 - 500 J/(kg·K) | ||
100.0 °C | 487 J/(kg·K) | ||
200.0 °C | 503 J/(kg·K) | ||
300.0 °C | 512 J/(kg·K) | ||
400.0 °C | 520 J/(kg·K) | ||
500.0 °C | 530 J/(kg·K) | ||
600.0 °C | 541 J/(kg·K) | ||
700.0 °C | 551 J/(kg·K) | ||
800.0 °C | 559 J/(kg·K) | ||
Thermal conductivity | -100.0 °C | 11.7 W/(m·K) | |
20.0 °C | 14.5 - 15 W/(m·K) | ||
100.0 °C | 16 W/(m·K) | ||
200.0 °C | 17.6 W/(m·K) | ||
300.0 °C | 19.1 W/(m·K) | ||
400.0 °C | 20.4 W/(m·K) | ||
500.0 °C | 21.9 W/(m·K) | ||
600.0 °C | 23.3 W/(m·K) | ||
700.0 °C | 24.7 W/(m·K) | ||
800.0 °C | 26.1 W/(m·K) | ||
Thermal diffusivity | -100.0 °C | 3.7 mm²/s | |
20.0 °C | 3.9 mm²/s | ||
100.0 °C | 4.3 mm²/s | ||
200.0 °C | 4.3 mm²/s | ||
300.0 °C | 4.6 mm²/s | ||
400.0 °C | 4.7 mm²/s | ||
500.0 °C | 4.9 mm²/s | ||
600.0 °C | 5 mm²/s | ||
700.0 °C | 5.3 mm²/s | ||
800.0 °C | 5.7 mm²/s | ||
Electrical
| Property | Temperature | Value |
|---|---|---|
Electrical resistivity | -100.0 °C | 5.86E-7 Ω·m |
20.0 °C | 6.92E-7 - 7.3E-7 Ω·m | |
100.0 °C | 7.58E-7 Ω·m | |
200.0 °C | 8.36E-7 Ω·m | |
300.0 °C | 9.07E-7 Ω·m | |
400.0 °C | 9.73E-7 Ω·m | |
500.0 °C | 1.02E-6 Ω·m | |
600.0 °C | 1.06E-6 Ω·m | |
700.0 °C | 1.1E-6 Ω·m | |
800.0 °C | 1.13E-6 Ω·m | |
Chemical properties
| Property | Value |
|---|---|
Carbon | 0.07 % |
Chromium | 17 - 19.5 % |
Manganese | 2 % |
Nickel | 8 - 10.5 % |
Nitrogen | 0.1 - 0.11 % |
Phosphorus | 0.05 % |
Silicon | 1 % |
Sulfur | 0.015 % |
Metal
- EN 10222-5 X2CrNiMo18-14-3 Solution‑Annealed Grade for Corrosion‑Resistant Applications
- EN 10269 X5CrNi18-10 Austenitic Stainless Steel – Solution Annealed with Annealing Treatment
- EN 10222‑5 X5CrNi18‑10 Solution Annealed (+AT): High‑Performance Austenitic Stainless Steel
- EN 10250-4 Grade X5CrNi18-10 Solution-Annealed Steel (+AT) – Premium Corrosion-Resistant Austenitic Alloy
- EN 10217-7 X5CrNi18-10 Austenitic Steel – Solution Annealed (+AT) for Corrosion Resistance
- EN 10216-5 Grade X5CrNi18-10 Solution Annealed (+AT) – High Corrosion Resistance Stainless Steel
- EN 10028-7 Grade X2CrNiMo18-14-3 – Solution-Annealed Stainless Steel with Superior Corrosion Resistance
- EN 10272 Grade X5CrNi18-10 Solution-Annealed Steel (+AT): Premium Austenitic Steel for Pressure Vessels
- EN 10028-7 Grade X5CrNi18-10 Solution Annealed (+AT) – High-Performance Austenitic Stainless Steel
- EN 10028-7 X6CrNiTi18-10 Solution-Annealed Steel: High-Temp, Corrosion-Resistant, Pressure Vessel & Civil Engineering Grade