DIN 17440 Grade X2CrNiMo18-14-3 Quenched Steel – Superior Corrosion Resistance for Chemical, Textile, Pharma Equipment

Properties: - modification of 1.4404 with higher chromium, nickel and molybdenum content - therefore improved corrosion properties Application: - in the apparatus engineering of the chemical industry, cellulose, textile and pharmaceutical industry

Quantity: 220,00€Additional services: Processing in our products

ALLEIMA (FORMERLY SANDVIK MATERIALS TECHNOLOGY)

MANUFACTURER

Information and services

Additional services: To ensure our customers' processes and/or products attain – and even exceed – their performance expectations, we offer a wide range of services within both the technical area and delivery logistics. Our technical services include: • Material consultations through our worldwide sales network • Advice in process optimization based on an in-depth applications knowledge • Joint new product development supported by our extensive R&D program View product groups and services

Properties

General

PropertyTemperatureValue

Density

20.0 °C

7.98 - 8.01 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

-100.0 °C

206 GPa

20.0 °C

196 - 200 GPa

100.0 °C

190 - 194 GPa

200.0 °C

182 - 186 GPa

300.0 °C

174 - 179 GPa

400.0 °C

166 - 172 GPa

500.0 °C

158 - 165 GPa

600.0 °C

150 GPa

700.0 °C

142 GPa

800.0 °C

134 GPa

Elongation

20.0 °C

30 - 40 %

Elongation A80

20.0 °C

35 %

Elongation A80, transverse

20.0 °C

40 %

Elongation, transverse

20.0 °C

30 - 40 %

Poisson's ratio

20.0 °C

0.28 [-]

Shear modulus

20.0 °C

77.3 GPa

Tensile strength

20.0 °C

490 - 690 MPa

Tensile strength, transverse

20.0 °C

490 - 690 MPa

Yield strength Rp0.2

20.0 °C

190 MPa

50.0 °C

182 MPa

100.0 °C

166 MPa

150.0 °C

152 MPa

200.0 °C

137 MPa

250.0 °C

127 MPa

300.0 °C

118 MPa

350.0 °C

113 MPa

400.0 °C

108 MPa

450.0 °C

103 MPa

500.0 °C

100 MPa

550.0 °C

98 MPa

Yield strength Rp0.2, transverse

20.0 °C

190 MPa

Yield strength Rp1.0

20.0 °C

225 MPa

50.0 °C

217 MPa

100.0 °C

199 MPa

150.0 °C

181 MPa

200.0 °C

167 MPa

250.0 °C

157 MPa

300.0 °C

145 MPa

350.0 °C

139 MPa

400.0 °C

135 MPa

450.0 °C

130 MPa

500.0 °C

128 MPa

550.0 °C

127 MPa

Yield strength Rp1.0, transverse

20.0 °C

225 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

-100.0 °C

1.49E-5 1/K

20.0 °C

1.61E-5 1/K

100.0 °C

1.65E-5 - 1.67E-5 1/K

200.0 °C

1.72E-5 - 1.75E-5 1/K

300.0 °C

1.75E-5 - 1.77E-5 1/K

400.0 °C

1.81E-5 - 1.85E-5 1/K

500.0 °C

1.84E-5 - 1.85E-5 1/K

600.0 °C

1.88E-5 1/K

700.0 °C

1.91E-5 1/K

800.0 °C

1.94E-5 1/K

900.0 °C

1.97E-5 1/K

1000.0 °C

2E-5 1/K

Melting point

1230 - 1480 °C

Typical for Austenitic Stainless Steel

Specific heat capacity

-100.0 °C

440 J/(kg·K)

20.0 °C

472 - 500 J/(kg·K)

100.0 °C

487 J/(kg·K)

200.0 °C

503 J/(kg·K)

300.0 °C

512 J/(kg·K)

400.0 °C

520 J/(kg·K)

500.0 °C

530 J/(kg·K)

600.0 °C

541 J/(kg·K)

700.0 °C

551 J/(kg·K)

800.0 °C

559 J/(kg·K)

900.0 °C

565 J/(kg·K)

1000.0 °C

571 J/(kg·K)

Thermal conductivity

20.0 °C

13.5 - 15 W/(m·K)

100.0 °C

14.9 W/(m·K)

200.0 °C

16.7 W/(m·K)

300.0 °C

18.3 W/(m·K)

400.0 °C

19.8 W/(m·K)

500.0 °C

21.3 W/(m·K)

600.0 °C

22.7 W/(m·K)

700.0 °C

24.2 W/(m·K)

800.0 °C

25.6 W/(m·K)

Thermal diffusivity

20.0 °C

3.6 mm²/s

100.0 °C

3.7 mm²/s

200.0 °C

4 mm²/s

300.0 °C

4.4 mm²/s

400.0 °C

4.6 mm²/s

500.0 °C

4.7 mm²/s

600.0 °C

4.9 mm²/s

700.0 °C

5.2 mm²/s

800.0 °C

5.5 mm²/s

Electrical

PropertyTemperatureValue

Electrical resistivity

20.0 °C

7.5E-7 - 7.75E-7 Ω·m

100.0 °C

8.42E-7 Ω·m

200.0 °C

9.04E-7 Ω·m

300.0 °C

9.62E-7 Ω·m

400.0 °C

1.01E-6 Ω·m

500.0 °C

1.06E-6 Ω·m

600.0 °C

1.1E-6 Ω·m

700.0 °C

1.13E-6 Ω·m

800.0 °C

1.16E-6 Ω·m

Chemical properties

PropertyValue

Carbon

0.03 %

Chromium

17 - 19 %

Manganese

2 %

Molybdenum

2.5 - 3 %

Nickel

12.5 - 15 %

Nitrogen

0.11 %

Phosphorus

0.05 %

Silicon

1 %

Sulfur

0.015 - 0.025 %


Metal

  1. X3CrNiMo17-13-3 Grade Steel (Quenched +Q) – DIN 17440 Certified for Pressure Vessels
  2. DIN 17440 X10CrNiS18-9 Quenched Steel – High-Performance Free-Cutting Alloy
  3. DIN 17440 X5CrNi18-12 Alloy Steel – Quenched +Q: High Corrosion Resistance & Strength
  4. DIN 1654‑5: X6CrNiMoTi17‑12‑2 Quenched Steel – Premium Cold‑Forming & Corrosion Resistance
  5. DIN 17440 Grade X2CrNiMoN17-12-2 Quenched: Premium Austenitic Steel for Chemical & Textile Industries
  6. DIN 17440 Grade X5CrNiMo17-13-3 (Q) – High-Performance Stainless Steel for Chemical Applications
  7. DIN 17440 X2CrNiMo18-16-4 Quenched Steel – Superior Corrosion Resistance & Precision Formability
  8. DIN 17440 X2CrNiMo18-14-3 Alloy: Heat‑Treated & Quenched for Superior Corrosion Resistance
  9. DIN 17440 Grade X6CrNiNb18-10 Quenched Steel – Superior Corrosion Resistance & High Temperature Performance
  10. DIN 17440 Grade X5CrNi18-10 Quenched: High-Performance Austenitic Steel for Corrosion-Resistant Applications