The austenitic steel X2CrNiMo18-15-4 is available in the solution annealed condition. Welded circular tubes of this steel are used for compression load and for corrosive load at room temperature, low temperatures and elevated temperatures. The material is resistant to intercrystalline corrosion (up
The austenitic steel X2CrNiMo18-14-3 is available in the solution annealed condition. Welded circular tubes of this steel are used for compression load and for corrosive load at room temperature, low temperatures and elevated temperatures. The material is resistant to intercrystalline corrosion (up
The austenitic steel X2CrNiMo17-12-2 is available in the solution annealed condition. Welded circular tubes of this steel are used for compression load and for corrosive load at room temperature, low temperatures and elevated temperatures. The material is resistant to intercrystalline corrosion (up
The austenitic steel X2CrNi19-11 is available in the solution annealed condition. Welded circular tubes of this steel are used for compression load and for corrosive load at room temperature, low temperatures and elevated temperatures. The material is resistant to intercrystalline corrosion (up to 3
The austenitic steel X1NiCrMoCu31-27-4 is available in the solution annealed condition. Welded circular tubes of this steel are used for compression load and for corrosive load at room temperature, low temperatures and elevated temperatures. The material is resistant to intercrystalline corrosion (u
The austenitic steel X1NiCrMoCu25-20-5 is available in the solution annealed condition. Welded circular tubes of this steel are used for compression load and for corrosive load at room temperature, low temperatures and elevated temperatures. The material is resistant to intercrystalline corrosion (u
CuZn36 (CW507L) is an unhardenable wrought alloy. High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are lower than for CuZn33. Corrosion resistance is similar to pure copper. Processing properties: warm forming: good cold forming: very goo
CuZn30 (CW505L) is an unhardenable wrought alloy. High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are lower than for CuZn28. Corrosion resistance is similar to pure copper. Processing properties: warm forming: good cold forming: very goo
CuZn20 (CW503L) is an unhardenable wrought alloy. High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are worse than for CuZn15. Corrosion resistance is similar to pure copper. Processing properties: warm forming: moderately cold forming: go
Fully austenitic, high temperature special steel, creep resistant up to approximately 800 degrees C, resistant to scaling up to 750 degrees C. It is insensitive to inclination to embrittlement. It is used for heat work tools as well as a component in hydrogenation plants that is resistant to pressur
Precipitation hardening, austenitic high temperature special steel which is resistant to scaling up to 750 degrees C and is creep resistant up to 650 degrees C. Used in steam boiler and turbine construction, in the chemical and petrochemical industries, for pipes in power plant construction. In the
CuZn10 (CW501L) is an unhardenable wrought alloy. High hardness and strength parameter are achievable by cold forming only. Thermal conductivity is lower than for CuZn5. Favorable electrical conductivity. Corrosion resistance is similar to pure copper. Processing properties: warm forming: moderatel
CuZn10 (CW501L) is an unhardenable wrought alloy. High hardness and strength parameter are achievable by cold forming only. Thermal conductivity is lower than for CuZn5. Favorable electrical conductivity. Corrosion resistance is similar to pure copper. Processing properties: warm forming: moderatel
The non-stabilised corrosion resistant austenitic steel X6CrNi18-10 (1.4948) is heat resistant up to 650 °C. Application mainly in the reactor engineering (Na-cooling circuits in fast breeders), in the steam boiler engineering as well as for pressure vessels and fastener parts. Acc. to DIN EN 1095 :
The ferritic steel X6CrNiTi12 is used in the annealed condition for cold rolled strip as well as for hot rolled strip and sheet.PropertiesGeneralPropertyTemperatureValueDensity20.0 °C7.7 g/cm³MechanicalPropertyTemperatureValueCommentElastic modulus20.0 °C220 GPa100.0 °C215 GPa200.0 °C210 GPa300.0 °C
X3CrNiMo17-13-3 is an austenitic steel that is resistant to intercrystalline corrosion. Temperature of solution is between 1020 and 1200°C (max. temperature is a reference data) and is cooled in water or air.PropertiesGeneralPropertyTemperatureValueDensity20.0 °C8 g/cm³MechanicalPropertyTemperatureV
The austenitic steel X2CrNi18-9 is available in solution annealed condition in the form of cold rolled strip, warm rolled strip and warm rolled sheet. The material is resistant to intercrystalline corrosion also in welded condition.PropertiesGeneralPropertyTemperatureValueDensity20.0 °C7.9 g/cm³Mech
The austenitic steel X6CrNi25-20 is applicated for high temperature resistant construction parts. The material is not resistant to intercrystalline corrosion. The steel is according to DIN EN 10095 usable as heat resistant steel.PropertiesGeneralPropertyTemperatureValueDensity20.0 °C7.9 g/cm³Mechani
The high corrosion resistant austenitic steel X1CrNiMoCuN 20 18 7 (new designation: X1CrNiMoCuN20-18-7), mat. number 1.4547, is applicable for pressure vessels acc. to TRB 100 and pipeline systems acc. to TRB 100 as well as AD-data sheet W 2 and W 10 from -60 to 400 deg., for steam boilers as per TR
The austenitic steel X6CrNi23-13 is applicated for high temperature resistant parts. The material is not resistant to intercrystalline corrosion. The steel is according to DIN EN 10095 usable as heat resistant steel.PropertiesGeneralPropertyTemperatureValueDensity20.0 °C7.9 g/cm³MechanicalPropertyTe